Fatigue behavior of Y-TZP ceramic after surface treatments

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Grinding and Resintering on the Fatigue Limit and Surface Characterization of a Y-TZP Ceramic.

This study evaluated the effect of grinding protocols and resintering on flexural fatigue limit and surface characterization of LavaTM Y-TZP. Bar-shaped specimens (20×4.0×1.2 mm, n=40; 20×4.0×1.5 mm, n=80) were obtained. Half of the thinner specimens (1.2 mm) constituted the as-sintered group (AS), while the thicker ones (1.5 mm) were ground with diamond burs under irrigation (WG) or not (G). T...

متن کامل

Low temperature degradation of a Y-TZP dental ceramic.

Bars of Y-TZP ceramic for dental restorations were subjected to hydrothermal degradation via in vitro exposure to water steam at 140°C for 7 days. X-ray diffraction, atomic force microscopy and scanning electron microscopy techniques were applied to observe and quantify the tetragonal-monoclinic (t-m) phase transformation associated with the process. Nanoindentation was used to assess the ceram...

متن کامل

Ceramic Processing Research Densification behavior of Y-TZP containing zirconium diboride composites

M. Amiriyan, S. Ramesh*, R. Tolouei, W.J. Kelvin Chew, J. Purbolaksono, M.A. Hassan, M. Hamdi and W.D. Teng Faculty of Science and Engineering, Laval University, Quebec, G1V 0A6 Canada Centre of Advanced Manufacturing & Material Processing (AMMP), Department of Engineering Design and Manufacture, Faculty of Engineering, University of Malaya, 50603 Kuala Lumpur, Malaysia Ceramics Technology Grou...

متن کامل

Fracture Resistance and Surface Treatment of Y-tzp Prepable Ceramic Abutments and Bars

NIMET DIAMOND ADATIA Fracture Resistance And Surface Treatment Of Y-TZP Prepable Ceramic Abutments and Bars. (Under the direction of Dr. Stephen Bayne) Intraoral preparation of zirconia implant abutments creates deep surface defects making abutments susceptible to fracture during loading. Fracture strengths were tested for (1) HIP-processed zirconia bars (Astra-Tech) after preparation and/or su...

متن کامل

Improvement in the Tensile Bond Strength between 3Y-TZP Ceramic and Enamel by Surface Treatments

This study examined the effects of 3 mol % yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) ceramic surface treatments on the tensile bond strength and surface characteristics of enamel. To measure the tensile bond strength, the 3Y-TZP and tooth specimens were manufactured in a mini-dumbbell shape and divided into four groups based on the type of 3Y-TZP surface treatment: polishing (P...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Mechanical Behavior of Biomedical Materials

سال: 2016

ISSN: 1751-6161

DOI: 10.1016/j.jmbbm.2015.11.042