Fatigue and Fracture Behaviours of FSW and FSP Joints of AA5083-H111 Aluminium Alloy

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue and Anisotropic behaviours of cold rolled AA1200 Aluminium Alloy

This study examines the fatigue and anisotropy behaviour of cold rolled AA1200 aluminium alloy for light weight automotive connecting rod application. Aluminium (Al) 1200 ingots were melted at temperature of 680 0C (after one hour of heating) cast in sand mould and cast samples homogenized for 6 hrs at 480 0C. The cold rolling process was carried out after homogenisation for 10, 20, 30, 40 and ...

متن کامل

Fatigue Strength Estimation Based on Local Mechanical Properties for Aluminum Alloy FSW Joints

Overall fatigue strengths and hardness distributions of the aluminum alloy similar and dissimilar friction stir welding (FSW) joints were determined. The local fatigue strengths as well as local tensile strengths were also obtained by using small round bar specimens extracted from specific locations, such as the stir zone, heat affected zone, and base metal. It was found from the results that f...

متن کامل

The Effects of Surface Pretreatment on the Cyclic-Fatigue Characteristics of Bonded Aluminium-Alloy Joints

The present work has used an accelerated test method, based upon cyclic-fatigue testing using a fracture-mechanics approach, to study the durability of organosilanepretreated joints which were adhesively-bonded using a hot-cured epoxy-film adhesive. The silane primer investigated was γ-glycidoxypropyltrimethoxysilane (GPS). The cyclic-fatigue tests were mainly conducted in (a) a ‘dry’ environme...

متن کامل

postnatal studies of bats (pipistrellus kuhlii and miniopterus schreibersii) & histomorphology and histochemistry studies of organs and diseases of (neurergus microspilotus and n. kaiseri)

1. to determine whether difference in birth body mass influenced growth performance in pipistrellus kuhlii we studied a total of 12 captive-born neonates. bats were assigned to two body mass groups: light birth body mass (lbw: 0.89 ± 0.05, n=8) and heavy birth body mass (hbw: 1.35 ± 0.08, n=4). heavier body mass at birth was associated with rapid postnatal growth (body mass and forearm length) ...

TENSILE AND FRACTURE CHARACTERISTICS OF A SIC- PARTICLE-REINFORCED 7075 ALUMINIUM ALLOY

Fracture behavior of a 7075 aluminium alloy reinforced with 15 Vol%. SiC particles was studied after T6 and annealing heat treatments under uniaxial tensile loading at room temperature. The scanning electron microscopy of fractured surfaces and EDS analysis showed:, that fracture mechanism changed from due mainly to fractured particle in T6 condition to interface decohesion in samples in anneal...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: IOP Conference Series: Materials Science and Engineering

سال: 2018

ISSN: 1757-899X

DOI: 10.1088/1757-899x/454/1/012055