Fast testing of ambient temperature pitting corrosion in type 2205 duplex stainless steel by bipolar electrochemistry experiments

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

IMPROVING PITTING CORROSION OF 304 STAINLESS STEEL BY ELECTROPOLISHING TECHNIQUE

Several surface modification techniques such as ion implantation, surface laser melting, have been employed to improve pitting corrosion resistance of stainless steel. Electropolishing is a technique in which the surface roughness is eliminated through a selective electrochemical dissolution. The effect of electropolishing on pitting corrosion of 304 stainless steel (SS) was investigated employ...

متن کامل

Study on Static Recrystallization Process in Duplex Stainless Steel 2205

Steel 2205 is one of the most famous duplex stainless steels. The microstructure of this steel composed of ferrite and austenite in similar amount. Therefore, in order to improve mechanical properties through microstructure, thermo mechanical processes such as controlled hot rolling and forging should be applied. It is not possible to employ the usual heat treatment. It shows the importance of ...

متن کامل

Corrosion Resistance and Semiconducting Properties of the Passive Films on Duplex Stainless Steel 2205

In this study, the effect of molybdate on the electrochemical behavior and semi-conductive properties of duplex stainless steel 2205 passive film at NaCl solutions was investigated. Cyclic potentiodynamic polarization, impedance spectroscopy, mott-schottky plots and scanning electron microscopy (SEM) were used to study the passive behavior. Polarization curves showed that the corrosion current ...

متن کامل

DETERIORATION OF PITTING CORROSION OF 316 STAINLESS STEEL BY SENSITIZATION HEAT TREATMENT

In this research pitting Corrosion of a sensitized 316 stainless steel was investigated employing potentiodynamic, potentiostatic techniques. Sensitization process was carried out on as-received alloy by submitting the specimen in electric furnace set at 650°Cfor five hours and then the specimen was quenched 25°C water. Potentiodynamic polarization of as received and sensitized specimens in 1M ...

متن کامل

study on static recrystallization process in duplex stainless steel 2205

steel 2205 is one of the most famous duplex stainless steels. the microstructure of this steel composed of ferrite and austenite in similar amount. therefore, in order to improve mechanical properties through microstructure, thermo mechanical processes such as controlled hot rolling and forging should be applied. it is not possible to employ the usual heat treatment. it shows the importance of ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Electrochemistry Communications

سال: 2020

ISSN: 1388-2481

DOI: 10.1016/j.elecom.2020.106779