In recent years, the interest in light metals has increased due to increasing demand for components with high specific strength and long service life industry. this context, titanium alloys have become very common popular owing their strength/weight properties superior refractory characteristics. study, effect of boundary condition tapered angle on natural frequency vibration behavior beam was investigated Ti-6Al-4V beams coated three different ceramic materials; Al2O3, AlN, TiB2. Tapered values are considered as 0°, 0.2°, 0.4°, 0.6° 0.8°. Besides, conditions were evaluated two including left side fixed or both sides fixed. All analyzes performed finite element-based Ansys APDL 19 program. According results obtained from analyses, it observed that there a change according type coating material, but no difference found terms increase/decrease tendency. addition, resultant displacement determined all samples. The indicated severely affected by angle. A decreasing trend samples

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue of Ti-6Al-4V

Metallic biomaterials have essentially three fields of use; these are the artificial hip joints, screw, plates and nails for internal fixation of fractures, and dental implants. Any of these devices must support high mechanical load and resistance of material against breakage is essential. High mechanical properties are needed for structural efficiency of surgical and dental implants. But their...

متن کامل

Durability of Fe-Co Thin Films on Ti-6Al-4V

The durability of Fe-Co thin films bonded on Ti-6Al-4V was studied as a function of layer thickness at ambient temperature. Interface toughness of the thin films was characterized by indentation and analyzed using an interface fracture model. The critical stresses for interface debonding and the fatigue life response of Ti-6Al-4V with and without Fe-Co thin films were evaluated by three-point b...

متن کامل

Precision Grinding of Titanium (Ti-6Al-4V) Alloy Using Nanolubrication

In this current era of competitive machinery productions, the industries are designed to place more emphasis on the product quality and reduction of cost whilst abiding by the pollution-preventing policy. In attempting to delve into the concerns, the industries are aware that the effectiveness of existing lubrication systems must be improved to achieve power-efficient and pollutionpreventing ma...

متن کامل

Notch Corrosion Fatigue Behavior of Ti-6Al-4V

The aim of this paper is to map the corrosion fatigue characteristics of Ti-6Al-4V alloy through the evaluation of the corrosion fatigue initiation and failure mechanisms. The study included the effect of the stress concentration factor at very high Kt values and the role of different inert or corrosive environments. This alloy is widely used in naval-structures and aero-engine communities and ...

متن کامل

Tensile fracture during transformation superplasticity of Ti–6Al–4V

During thermal cycling through the a–b phase transformation under the action of a small external biasing stress, Ti alloys exhibit an average deformation stress exponent of unity and achieve superplastic strains. We report tensile experiments on Ti–6Al–4V with an applied stress of 4.5 MPa, aimed at understanding the failure processes during transformation superplasticity. The development of cav...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Ni?de Ömer Halisdemir Üniversitesi mühendislik bilimleri dergisi

سال: 2022

ISSN: ['2564-6605']

DOI: https://doi.org/10.28948/ngumuh.1078779