Fabrication of Ti/TiO2 and Cu/TiO2 Composite Photocatalyst by Spark Plasma Sintering and its Characteristics
نویسندگان
چکیده
منابع مشابه
Fabrication of Nanostructured Cu matrix Nanocomposites by High Energy Mechanical Milling and Spark Plasma Sintering
Spark plasma sintering (SPS) is a sintering process that is capable of sintering hard worked powders in short times. This technique was used to fabricate bulk Cu and Cu-SiC nanocomposites. Pure Cu and mixed powders of Cu including 4 vol% of SiC nanoparticles were mechanically alloyed for 25 h and sintered at 750˚C under vacuum condition by SPS method. Microstructures of the materials were chara...
متن کاملFabrication and Characteristics of 8YSZ/Ni functionally Graded Materials by Applying Spark Plasma Sintering Procedure (RESEARCH NOTE)
Functionally graded materials (FGM) in the form of layered structure consisting of yttria stabilized zirconia (8 mol% Y2O3) and nickel were fabricated by spark plasma sintering procedure. The relative density, linear shrinkage and Vickers hardness of each layer of graded materials were measured. The microstructure and the composition of these components were studied. The results obtained show t...
متن کاملIN SITU FABRICATION OF Al 2024-Mg2Si COMPOSITE BY SPARK PLASMA SINTERING OF REACTIVE MECHANICALLY ALLOYED POWDER
In situ Al2024- Mg2Si composite was fabricated by spark plasma sintering (SPS) of reactive powder. Reactive powder was obtained from mechanical alloying (MA) of elemental powders. Clad layers of in situ composite were fabricated on Al substrates by spark plasma sintering (SPS). Structural evolution during MA process and after SPS was investigated by X-ray diffractometery (XRD). Scanning electro...
متن کاملIn-situ Fabrication of Transparent Magnesium Aluminate Spinel by Spark Plasma Sintering
Transparent polycrystalline spinel ceramic was fabricated without any sintering aids by spark plasma sintering method of a mixture of Al2O3 and MgO powders for only 10min soak at 1250°C. Densification, microstructure and optical transparency of spinel were examined. The spinel exhibits an in-line transmission of 55% for a visible-wavelength of 470nm and high hardness value of 2040 HV.
متن کاملComparison of Creep Behavior in Alumina Based Ceramics Densified by Spark Plasma Sintering and Hot Pressing
Spark plasma sintering (SPS) method, as plasma activated sintering, is a method applicable for rapid sintering of metals and ceramics. Owing to the advantage of rapid heating, the alumina ceramics obtained by SPS have a grain size and density comparable to those of hot pressed ones. The increase of densification rate may be related to some difference in ion transport characteristics. This study...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Society of Powder and Powder Metallurgy
سال: 2010
ISSN: 0532-8799,1880-9014
DOI: 10.2497/jjspm.57.69