Fabrication of Aluminum Borate Whisker Preform without Binder and Characteristics of 6061 Aluminum Alloy Matrix Composite

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Welding Aluminum Alloy 6061 with Opposing Dual Torch Gtaw Process

Cracking is a major concern in welding aluminum alloys. Although weld solidification cracks can be eliminated through addition of filler alloy, the additives modify the alloy or base-metal constituents and may not always be desirable. High-energy beam processes, such as electron-beam welding, that result in minimal heat input reduce crack sensitivity, but their high cost limits their applicatio...

متن کامل

Void growth in 6061-aluminum alloy under triaxial stress state

In numerous metals and alloys, ductile fracture involves void nucleation, growth, and coalescence. In this contribution, void growth has been quantitatively characterized in an extruded 6061-wrought Al-alloy as a function of stress state in notch tensile test specimens. Digital image analysis and Stereology have been used to estimate the volume fraction and three-dimensional number density of v...

متن کامل

Fabrication of synchronized hammer peening with pulsed laser welding and its effect on 6061 aluminum alloy weld

The non-continuous laser beam in pulsed lasers allows the mechanical peening between two consecutive beams on a still hot weld bead. At a very short time (20, 150 and 300 ms) after laser pulse application, mechanical peening was performed on the welding bead. To achieve these short times, the light sensor detects the nth laser pulse and the mechanical arm starts moving. Upon reaching the tip of...

متن کامل

Fabrication of synchronized hammer peening with pulsed laser welding and its effect on 6061 aluminum alloy weld

The non-continuous laser beam in pulsed lasers allows the mechanical peening between two consecutive beams on a still hot weld bead. At a very short time (20, 150 and 300 ms) after laser pulse application, mechanical peening was performed on the welding bead. To achieve these short times, the light sensor detects the nth laser pulse and the mechanical arm starts moving. Upon reaching the tip of...

متن کامل

Analysis of Surface Roughness and Micro-hardness in Roller Burnishing of Aluminum Alloy 6061

Burnishing is a chip-less finishing process, in which a hard roller or ball presses the surface layer of part to perform plastic deformation in the surface layer and produce improved finish, enhanced hardness and compressive residual stresses on the surface of special materials such as Aluminum and Brass. In the following research, the effect of input parameters such as feed rate, cutting speed...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Japan Institute of Metals and Materials

سال: 1994

ISSN: 0021-4876,1880-6880

DOI: 10.2320/jinstmet1952.58.1_78