Experimental and simulation study for rewelding defects during the flow process of Semi-solid die casting

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

simulation and experimental studies for prediction mineral scale formation in oil field during mixing of injection and formation water

abstract: mineral scaling in oil and gas production equipment is one of the most important problem that occurs while water injection and it has been recognized to be a major operational problem. the incompatibility between injected and formation waters may result in inorganic scale precipitation in the equipment and reservoir and then reduction of oil production rate and water injection rate. ...

Study of Process Parameters of Gravity Die Casting Defects

In today’s world a casting production without any defect is almost impossible. After the application of various optimization techniques and process we still are not able to get the defect free castings. So it is critically important to analyze the root cause of casting defect with in the process itself, so that any changes which can hamper the defect intensity can be invoked at the time of manu...

متن کامل

consequence analysis of the leakage, ignition and explosion during high pressure sour gas injection process to the oil reservoir

there is no doubt that human being needs to become integrated with industry and industry needs to be progressed, daily. on the other hand, serious events in industrial units specially in oil industries has been shown that such damages and events are industry related ones. the consequence of such events and damages which resulted in chemical and poisoned explosions and loss of life and property ...

Flow simulation of gallium in a cylindrical annulus in the presence of a magnetic field for improving the casting process

Free convection flow in an enclosure filled with a congealing melt leads to the product with a nonuniform structure involving large grains. The convective flows are decreased by applying an appropriate magnetic field, obtaining uniform and small grain structures. In this work, using the finite volume method, we investigated the application of a magnetic field to the convective heat transfer and...

متن کامل

study of cohesive devices in the textbook of english for the students of apsychology by rastegarpour

this study investigates the cohesive devices used in the textbook of english for the students of psychology. the research questions and hypotheses in the present study are based on what frequency and distribution of grammatical and lexical cohesive devices are. then, to answer the questions all grammatical and lexical cohesive devices in reading comprehension passages from 6 units of 21units th...

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Physics: Conference Series

سال: 2019

ISSN: 1742-6588,1742-6596

DOI: 10.1088/1742-6596/1347/1/012124