Evidence of High-Temperature Strain Heterogeneities in a Nickel-Based Single-Crystal Superalloy
نویسندگان
چکیده
منابع مشابه
High Temperature Deformation Mechanisms in a DLD Nickel Superalloy
The realisation of employing Additive Layer Manufacturing (ALM) technologies to produce components in the aerospace industry is significantly increasing. This can be attributed to their ability to offer the near-net shape fabrication of fully dense components with a high potential for geometrical optimisation, all of which contribute to subsequent reductions in material wastage and component we...
متن کاملPreferred growth orientation and microsegregation behaviors of eutectic in a nickel-based single-crystal superalloy
A nickel-based single-crystal superalloy was employed to investigate the preferred growth orientation behavior of the (γ + γ') eutectic and the effect of these orientations on the segregation behavior. A novel solidification model for the eutectic island was proposed. At the beginning of the eutectic island's crystallization, the core directly formed from the liquid by the eutectic reaction, an...
متن کاملModelling plastic deformation in a single-crystal nickel-based superalloy using discrete dislocation dynamics
Background: Nickel-based superalloys are usually exposed to high static or cyclic loads in non-ambient environment, so a reliable prediction of their mechanical properties, especially plastic deformation, at elevated temperature is essential for improved damage-tolerance assessment of components. Methods: In this paper, plastic deformation in a single-crystal nickel-based superalloy CMSX4 at el...
متن کاملCrystal plasticity and crack initiation in a single-crystal nickel-base superalloy Modelling, evaluation and applications
In this dissertation the work done in the projects KME-410/502 will be presented. The overall objective in these projects is to evaluate and develop tools for designing against fatigue in single-crystal nickel-base superalloys in gas turbines. Experiments have been done on single-crystal nickel-base superalloy specimens in order to investigate the mechanical and fatigue behaviour of the materia...
متن کاملEffect of Thermal History on Microstructural Changes in Aluminized Nickel-Based Single-Crystal Superalloy
The effect of the thermal history on microstructural changes in aluminized and Pt-aluminized Ni-based single-crystal superalloys was investigated. The superalloy substrates were first electropolished to get rid of the residual surface strain. Then, Pt was electrodeposited and vacuum annealing was conducted for some of the substrates, and aluminized and Pt-aluminized specimens were prepared usin...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Advanced Engineering Materials
سال: 2013
ISSN: 1438-1656
DOI: 10.1002/adem.201300016