Evaluation of TiO2 and ZnO atomic layer deposition coated polyamide 66 fabrics for photocatalytic activity and antibacterial applications
نویسندگان
چکیده
منابع مشابه
The Antibacterial Polyamide 6-ZnO Hierarchical Nanofibers Fabricated by Atomic Layer Deposition and Hydrothermal Growth
In this paper, we report the combination of atomic layer deposition (ALD) with hydrothermal techniques to deposit ZnO on electrospun polyamide 6 (PA 6) nanofiber (NF) surface in the purpose of antibacterial application. The micro- and nanostructures of the hierarchical fibers are characterized by field emission scanning electron microscopy (FE-SEM), high-resolution transmission electron microsc...
متن کاملPhotocatalytic Properties of Co3O4-Coated TiO2 Powders Prepared by Plasma-Enhanced Atomic Layer Deposition
Co3O4-coated commercial TiO2 powders (P25) p-n junction photocatalysts were prepared by plasma-enhanced atomic layer deposition (PEALD) technique. The structure, morphology, bandgap, and photocatalytic properties under ultraviolet light were investigated systematically. Although the deposition of Co3O4 does not change the anatase structure and crystallite size of P25 powders, the ultraviolet ph...
متن کاملMicroscopic Study of Atomic Layer Deposition of TiO2 on GaAs and Its Photocatalytic Application
We report a microscopic study of p-GaAs/TiO2 heterojunctions using cross-sectional high resolution transmission electron microscopy (HRTEM). The photocatalytic performance for both H2 evolution and CO2 reduction of these heterostructures shows a very strong dependence on the thickness of the TiO2 over the range of 0−15 nm. Thinner films (1−10 nm) are amorphous and show enhanced catalytic perfor...
متن کاملSynthesis of Pt@TiO2@CNTs Hierarchical Structure Catalyst by Atomic Layer Deposition and Their Photocatalytic and Photoelectrochemical Activity
Pt@TiO2@CNTs hierarchical structures were prepared by first functionalizing carbon nanotubes (CNTs) with nitric acid at 140 °C. Coating of TiO2 particles on the CNTs at 300 °C was then conducted by atomic layer deposition (ALD). After the TiO2@CNTs structure was fabricated, Pt particles were deposited on the TiO2 surface as co-catalyst by plasma-enhanced ALD. The saturated deposition rates of T...
متن کاملOptical and microstructural properties of ZnO/TiO2 nanolaminates prepared by atomic layer deposition
ZnO/TiO2 nanolaminates were grown on Si (100) and quartz substrates by atomic layer deposition at 200°C using diethylzinc, titanium isopropoxide, and deionized water as precursors. All prepared multilayers are nominally 50 nm thick with a varying number of alternating TiO2 and ZnO layers. Sample thickness and ellipsometric spectra were measured using a spectroscopic ellipsometer, and the parame...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Vacuum Science & Technology A
سال: 2021
ISSN: 0734-2101,1520-8559
DOI: 10.1116/6.0000761