Evaluation of thermo-mechanical fatigue crack propagation behavior of Ni-based single crystal superalloy CMSX-4
نویسندگان
چکیده
منابع مشابه
Effect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy
Effect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy Xingbo Liu a,*, ling Xu a, Ever Barbero a, Wei-Di Cao b, Richard L. Kennedy b a West Virginia University, Morgantown, WV 26506-6106, USA b Allvac, an AT! Technologies Company, Monroe, NC 28111-5030, USA Received 22 October 2006; received in revised form 23 March 2007; accepted 10 May 2007 The effec...
متن کاملFatigue crack initiation in a notched single-crystal superalloy component
In this paper, the fatigue crack initiation in notched single-crystal test specimens of material MD2 is investigated and analysed. A critical plane approach is adopted, in which the total strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to describe the number of cycles to fatigue crack initiation. This relation is determined from a...
متن کاملThermo-Mechanical Fatigue Crack Growth of RR1000
Non-isothermal conditions during flight cycles have long led to the requirement for thermo-mechanical fatigue (TMF) evaluation of aerospace materials. However, the increased temperatures within the gas turbine engine have meant that the requirements for TMF testing now extend to disc alloys along with blade materials. As such, fatigue crack growth rates are required to be evaluated under non-is...
متن کاملEvaluation of Fatigue Crack Initiation in a Notched Single-crystal Superalloy Component
The fatigue crack initiation in a notched single-crystal nickel-base superalloy component at 500°C was investigated and analysed. A critical plane approach in combination with a critical distance method has been adopted, in which the total shear strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to predict the number of cycles to fat...
متن کاملAn Empirical Approach to Correlating Thermo-Mechanical Fatigue Behaviour of a Polycrystalline Ni-Base Superalloy
Assessment of thermo-mechanical fatigue behaviour of the polycrystalline nickel alloy RR1000 reveals a significant effect of phase angle on fatigue life. The current paper explores two scenarios: the first where the mechanical strain range is held constant and comparisons of the fatigue life are made for different phase angle tests; and secondly, the difference between the behaviour of In-phase...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Transactions of the JSME (in Japanese)
سال: 2014
ISSN: 2187-9761
DOI: 10.1299/transjsme.2014smm0294