Enhancing Surface Topology of Udimet®720 Superalloy through Ultrasonic Vibration-Assisted Ball Burnishing
نویسندگان
چکیده
منابع مشابه
Study of the lateral pass width for conventional and ultrasonic vibrations- assisted ball burnishing on Ti-6Al-4V specimens
Ball burnishing is a technological finishing process based on plastic deformation of the objective surface by means of a hard ball gliding over it. Along with its easiness of application, possible on the same machine where machining was performed [1], burnishing is a comprehensive process able to achieve surface roughness improvements, and compressive residual stresses up to deep layers of the ...
متن کاملUltrasonic Vibration Assisted Electro-Discharge Machining
An ultrasonic vibration has been superposed on the normal electrode movement to increase the flushing effect during a micro electro-discharge machining (EDM) process. A systematic study on the effects of ultrasonic vibration on the EDM performance for fabricating microholes in Nitinol has been completed. The introduction of ultrasonic vibration to the microEDM process has more than 60 times inc...
متن کاملDetermination of Surface Roughness by Ball Burnishing Process Using Factorial Techniques
Burnishing is a method of finishing and hardening machined parts by plastic deformation of the surface. Experimental work based on central composite second order rotatable design has been carried out on a lathe machine to establish the effects of ball burnishing parameters on the surface roughness of brass material. Analysis of the results by the analysis of variance technique and the F-test sh...
متن کاملvibration cutting and elliptical ultrasonic vibration assisted turning of in738 work-pieces
vibration cutting (vc), elliptical vibration cutting (evc) and ordinary cutting (oc) of in738 work-pieces have been experimentally investigated in the present research. the experiments were carried out by using single crystal diamond tool and ultra-precision cnc lathe. vibration frequency is 36.16khz and the amplitude is . the influence of various cutting parameters including cutting speed, fee...
متن کاملInvestigation of Sequential Cryogenic Hard Turning and Ball Burnishing Processes
K. Żak, W. Grzesik, M. Prażmowski, Opole University of Technology, Department of Manufacturing Engineering and Automation, Opole, Poland This paper presents a sequential machining process which incorporates CBN hard turning with cryogenic pre-cooling of the workpiece (CHT) and ball burnishing (BB). The main goal of this study was to select machining conditions enhancing the quality of parts mac...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Metals
سال: 2020
ISSN: 2075-4701
DOI: 10.3390/met10070915