Enhancement of pitting corrosion resistance for AA1050 processed by continuous closed die forging
نویسندگان
چکیده
منابع مشابه
Enhancement of hot forging die life using different methods
Forging dies at high temperatures are under contact pressure, variable mechanical loads and thermal shock, furthermore they should withstand wear and friction in a high level. So, in order to increase die life, the selection of die material, coating and hardness is essential. In this review, various methods used for die life enhancement such as carbide coating, using the super alloy stellite 6 ...
متن کاملOptimization of Flash, Billet Dimensions and Friction Factor in Closed Die Cold Forging Process
Three important parameters in designing a closed die for forging process are ratio of width to flash thickness, ratio of height to billet diameter and the friction factor. In this paper the influences of these parameters on the required force for the forging and percentage of die filling were investigated. It was found that by controlling the flash dimension, the material loss is reduced and t...
متن کاملIMPROVING PITTING CORROSION OF 304 STAINLESS STEEL BY ELECTROPOLISHING TECHNIQUE
Several surface modification techniques such as ion implantation, surface laser melting, have been employed to improve pitting corrosion resistance of stainless steel. Electropolishing is a technique in which the surface roughness is eliminated through a selective electrochemical dissolution. The effect of electropolishing on pitting corrosion of 304 stainless steel (SS) was investigated employ...
متن کاملAn Upper Bound Solution for Closed Die Forging of Sintered Polygon
The paper reports on an investigation into the various aspects of closed die cold forging of polygonal powder preforms, which have been compacted and sintered from atomized powder. It is found that for certain dimensional ratios of the preform the die pressure is minimum. An attempt has been made for the determination of the die pressures developed for given geometries of the disc during the cl...
متن کاملCharacterization of pitting corrosion in aluminum films by light scattering
We report a detailed study of the morphology of pits formed by corrosion of aluminum thin films using an in-plane light scattering technique. We show that the corrosion front of the Al thin film can be treated as a quasi-two-level random rough surface. Based on an elastic diffraction theory, we are able to determine the average depth, the area, and the density of pits, as well as the fractal di...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Materials Research and Technology
سال: 2020
ISSN: 2238-7854
DOI: 10.1016/j.jmrt.2020.09.065