Enhanced Stability of Organic Photovoltaics by Additional ZnO Layers on Rippled ZnO Electron-collecting Layer using Atomic Layer Deposition

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Enhanced band-edge photoluminescence from ZnO-passivated ZnO nanoflowers by atomic layer deposition

The ZnO nanoflowers were synthesized by reactive vapor deposition. A secondary nucleation in the stalk/leaves interface was suggested. The photoluminescence revealed that there were many oxygen vacancies in the nanoflowers. To tune the optical properties of ZnO nanoflowers, ZnO thin films with varying thicknesses were coated on the nanoflowers by atomic layer deposition, which can distinctly im...

متن کامل

On the environmental stability of ZnO thin films by spatial atomic layer deposition

• A submitted manuscript is the author's version of the article upon submission and before peer-review. There can be important differences between the submitted version and the official published version of record. People interested in the research are advised to contact the author for the final version of the publication, or visit the DOI to the publisher's website. • The final author version ...

متن کامل

Enhanced visible photoluminescence from ultrathin ZnO films grown on Si-nanowires by atomic layer deposition.

Bright room temperature visible emission is obtained in heterostructures consisting of approximately 3.5 nm thick ZnO ultrathin films grown on Si-nanowires produced by means of self-masking dry etching in hydrogen-containing plasma. The ZnO films were deposited on Si-nanowires by using atomic layer deposition (ALD) under an ambient temperature of 25 degrees C. The orders of magnitude enhancemen...

متن کامل

Improved performance of organic light-emitting diodes fabricated on Al-doped ZnO anodes incorporating a homogeneous Al-doped ZnO buffer layer grown by atomic layer deposition.

In this work, we investigated the use of a homogeneous Al-doped zinc oxide (AZO) buffer layer to improve the performance of an organic light-emitting diode (OLED) device fabricated on an AZO anode. For this, 10-nm-thick AZO buffer layers with Al doping concentrations of 3.1, 4.1, and 5.1 at % were grown on 140-nm-thick AZO anode films containing 2.1 at % Al by atomic layer deposition. The elect...

متن کامل

Bi-layer Channel AZO/ZnO Thin Film Transistors Fabricated by Atomic Layer Deposition Technique

This letter demonstrates bi-layer channel Al-doped ZnO/ZnO thin film transistors (AZO/ZnO TFTs) via atomic layer deposition process at a relatively low temperature. The effects of annealing in oxygen atmosphere at different temperatures have also been investigated. The ALD bi-layer channel AZO/ZnO TFTs annealed in dry O2 at 300 °C exhibit a low leakage current of 2.5 × 10-13A, I on/I off ratio ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Bulletin of the Korean Chemical Society

سال: 2014

ISSN: 0253-2964

DOI: 10.5012/bkcs.2014.35.2.353