Enhanced piezoelectric performance of the ZnO/AlN stacked nanofilm nanogenerator grown by atomic layer deposition

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

(Sn,Al)Ox Films Grown by Atomic Layer Deposition

Tin oxide (SnO2) is a transparent semiconductor with a wide band gap and electrical resistivity as low as 2 10 4 Ω 3 cm and high infrared reflectivity, over 90%. 4 These properties are achieved using n-type doping by substituting fluorine for about 1% of the oxygen. The low electrical resistance and optical transparency in SnO2 are widely used in applications such as solar cells, displays, touc...

متن کامل

Enhanced visible photoluminescence from ultrathin ZnO films grown on Si-nanowires by atomic layer deposition.

Bright room temperature visible emission is obtained in heterostructures consisting of approximately 3.5 nm thick ZnO ultrathin films grown on Si-nanowires produced by means of self-masking dry etching in hydrogen-containing plasma. The ZnO films were deposited on Si-nanowires by using atomic layer deposition (ALD) under an ambient temperature of 25 degrees C. The orders of magnitude enhancemen...

متن کامل

Introduction to (plasma-enhanced) atomic layer deposition

Film growth by the atomic layer deposition (ALD) method relies on alternate pulsing of the precursor gases and vapors into a vacuum chamber and their subsequent chemisorption on the substrate surface (Fig. 1) [1,2]. The different steps in the process are saturative such that ALD film growth is self-limiting yielding one submonolayer of film per deposition cycle. ALD has some unique characterist...

متن کامل

Spoof-like plasmonic behavior of plasma enhanced atomic layer deposition grown Ag thin films

The plasmonic behavior of Ag thin films produced by plasma enhanced atomic layer deposition (PEALD) has been investigated. We show that as-deposited flat PEALD Ag films exhibit unexpected plasmonic properties, and the plasmonic enhancement can differ markedly, depending on the microstructure of the Ag film. Electromagnetic field simulations indicate that this plasmonic behavior is due to air ga...

متن کامل

Effects of Annealing Ambient on the Characteristics of LaAlO3 Films Grown by Atomic Layer Deposition

We investigated the effects of different annealing ambients on the physical and electrical properties of LaAlO3 films grown by atomic layer deposition. Post-grown rapid thermal annealing (RTA) was carried out at 600 °C for 1 min in vacuum, N2, and O2, respectively. It was found that the chemical bonding states at the interfacial layers (ILs) between LaAlO3 films and Si substrate were affected b...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: APL Materials

سال: 2018

ISSN: 2166-532X

DOI: 10.1063/1.5057889