Energy Absorbed by Charpy Specimens of Sintered Iron
نویسندگان
چکیده
منابع مشابه
Certification of NIST Room Temperature Low-Energy and High-Energy Charpy Verification Specimens.
The possibility for NIST to certify Charpy reference specimens for testing at room temperature (21 °C ± 1 °C) instead of -40 °C was investigated by performing 130 room-temperature tests from five low-energy and four high-energy lots of steel on the three master Charpy machines located in Boulder, CO. The statistical analyses performed show that in most cases the variability of results (i.e., th...
متن کاملThe Effect of Microstructure on Estimation of the Fracture Toughness (KIC) Rotor Steel Using Charpy Absorbed Energy (CVN)
The proportional relationships between the Charpy absorbed energy (CVN) and the KIC values have been established for a wide variety of steels. Several formulae have been proposed that predict KIC from CVN. The purpose of this study is to investigate, by means of compact testing fracture toughness specimens, the effective role of microstructure for estimation of the fractur...
متن کاملImpact Toughness Modification of NIST Low-Energy Charpy Verification Specimens for Testing at Room Temperature
The possibility for the National Institute for Standards and Technology (NIST) to certify Charpy reference specimens for testing at room temperature (21 °C ± 1 °C) instead of −40 °C was investigated in a previous study, in which a slightly increased likelihood of specimen jamming was observed at the low-energy level (13 J to 20 J). Moreover, there is a concern that the higher impact toughness o...
متن کاملInevitable iron loss by human adolescents, with calculations of the requirement for absorbed iron.
In growing individuals, the requirement for absorbed iron consists of iron needed for growth and iron needed to replace inevitable iron loss. We were able to estimate inevitable iron loss by adolescents because total body iron of the adolescents had been enriched with the stable isotope, (58)Fe, as the result of earlier studies of iron absorption. During an interval beginning at least 1.56 y af...
متن کاملA NOVEL PROCEDURE FOR MEASURING THE IMPACT FRACTURE TOUGHNESS KId WITH PRECRACKED CHARPY SPECIMENS
A procedure i s presented f o r determining the impact f r a c t u r e toughness K w i t h precracked Charpy specimens wi thout performing any load measurements.'?he Kid-val ue i s obtained from preestabl ished impact response curves and a measurement o f t h e t ime-to-fracture. The measuring technique i s f u l l y dynamic and does not impose any r e s t r i c t i o n s on t h e t e s t condi...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Society of Powder and Powder Metallurgy
سال: 1974
ISSN: 0532-8799,1880-9014
DOI: 10.2497/jjspm.21.161