Emissivity at high temperature of Ni-based superalloys for the design of solar receivers for future tower power plants
نویسندگان
چکیده
In the framework of H2020 European project POLYPHEM, whose main objective is to improve flexibility and performance small-scale solar power plants, studies have been conducted on various nickel-based alloys for design receiver. Inconel 600 alloy used as a reference material in advanced manufacturing high temperature receivers but other oxidation resistant selected such 617, Haynes 230, HR120 Hastelloy X best candidate will be making prototype. Thus, two essential quantities, namely absorptivity α – higher better total hemispherical emissivity ε lower were measured vacuum under atmospheric air up 1400 K MEDIASE reactor installed at focus 1000 kW furnace. The reach α/ε ratio highest possible. measurement was made by direct method requiring true using bi-chromatic pyro-reflectometer that its radiance spectro-radiometry. Total data are presented same time microstructural (SEM, XRD) topographic (3D profilometry) characterizations allowing interpretation evolution with growth oxide layer. Finally, 230 chosen build
منابع مشابه
application of upfc based on svpwm for power quality improvement
در سالهای اخیر،اختلالات کیفیت توان مهمترین موضوع می باشد که محققان زیادی را برای پیدا کردن راه حلی برای حل آن علاقه مند ساخته است.امروزه کیفیت توان در سیستم قدرت برای مراکز صنعتی،تجاری وکاربردهای بیمارستانی مسئله مهمی می باشد.مشکل ولتاژمثل شرایط افت ولتاژواضافه جریان ناشی از اتصال کوتاه مدار یا وقوع خطا در سیستم بیشتر مورد توجه می باشد. برای مطالعه افت ولتاژ واضافه جریان،محققان زیادی کار کرده ...
15 صفحه اولinvestigating the feasibility of a proposed model for geometric design of deployable arch structures
deployable scissor type structures are composed of the so-called scissor-like elements (sles), which are connected to each other at an intermediate point through a pivotal connection and allow them to be folded into a compact bundle for storage or transport. several sles are connected to each other in order to form units with regular polygonal plan views. the sides and radii of the polygons are...
study of cohesive devices in the textbook of english for the students of apsychology by rastegarpour
this study investigates the cohesive devices used in the textbook of english for the students of psychology. the research questions and hypotheses in the present study are based on what frequency and distribution of grammatical and lexical cohesive devices are. then, to answer the questions all grammatical and lexical cohesive devices in reading comprehension passages from 6 units of 21units th...
conditional copula-garch methods for value at risk of portfolio: the case of tehran stock exchange market
ارزش در معرض ریسک یکی از مهمترین معیارهای اندازه گیری ریسک در بنگاه های اقتصادی می باشد. برآورد دقیق ارزش در معرض ریسک موضوع بسیارمهمی می باشد و انحراف از آن می تواند موجب ورشکستگی و یا عدم تخصیص بهینه منابع یک بنگاه گردد. هدف اصلی این مطالعه بررسی کارایی روش copula-garch شرطی در برآورد ارزش در معرض ریسک پرتفویی متشکل از دو سهام می باشد و ارزش در معرض ریسک بدست آمده با روشهای سنتی برآورد ارزش د...
High Temperature Nanoindentation of Ni-base Superalloys
Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Solar Energy Materials and Solar Cells
سال: 2021
ISSN: ['0927-0248', '1879-3398']
DOI: https://doi.org/10.1016/j.solmat.2021.111066