Electrodeposition and Pitting Corrosion of Aluminum-Manganese Alloys from Room Temperature Chloroaluminate Molten Salts

نویسندگان

چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Azoniaspiro salts: towards bridging the gap between room-temperature ionic liquids and molten salts.

In a continued effort to improve the suitability of ionic liquids in applications operating at raised temperatures, novel spirocyclic 'azoniaspiro' salts (with cations derived from five-, six-, seven- and eight-membered rings) are prepared and characterised. The structural and thermal properties of these salts are compared against those of established analogues. The stable geometries and ion pa...

متن کامل

The electrodeposition of zinc alloys from ionic liquid electrolytes

Electrodeposited zinc alloys have long been recognised as effective barrier and sacrificial coatings for ferrous substrates. The effect of alloying zinc with, in the main, more noble metals, has produced finishes of higher corrosion resistance than simply electrodeposited zinc. In this manner zinc alloys such as zinc-nickel, zinc-cobalt and zinc-iron are routinely electrodeposited on an industr...

متن کامل

Characterization of pitting corrosion in aluminum films by light scattering

We report a detailed study of the morphology of pits formed by corrosion of aluminum thin films using an in-plane light scattering technique. We show that the corrosion front of the Al thin film can be treated as a quasi-two-level random rough surface. Based on an elastic diffraction theory, we are able to determine the average depth, the area, and the density of pits, as well as the fractal di...

متن کامل

Conductivities of Room Temperature Molten Salts Containing ZnCl2, Measured by a Computerized Direct Current Method

The conductivities of the binary room-temperature molten salt (RTMS) systems ZnCl 2-N-nbutylpyridinium chloride (BPC), ZnCl2 -1-ethyl-3-methylimidazolium chloride (EMIC) and ZnCl2 benzyltriethylammonium chloride (BTEAC) have been measured at different temperatures and compositions by a d.c. four-probes method. The conductivities of the three RTMS are in the order ZnCl2-EMIC > ZnCl2-BPC > ZnCl2-...

متن کامل

Conductivities of Room Temperature Molten Salts Containing AICI3, Measured by a Computerized Direct Current Method

für Naturforschung in cooperation with the Max Planck Society for the Advancement of Science under a Creative Commons Attribution 4.0 International License. Dieses Werk wurde im Jahr 2013 vom Verlag Zeitschrift für Naturforschung in Zusammenarbeit mit der Max-Planck-Gesellschaft zur Förderung der Wissenschaften e.V. digitalisiert und unter folgender Lizenz veröffentlicht: Creative Commons Namen...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: ECS Proceedings Volumes

سال: 1999

ISSN: 0161-6374,2576-1579

DOI: 10.1149/199941.0517pv