Electrical tuning of the spin–orbit interaction in nanowire by transparent ZnO gate grown by atomic layer deposition

نویسندگان

چکیده

We develop an InAs nanowire gate-all-around field-effect transistor using a transparent conductive zinc oxide (ZnO) gate electrode, which is in-situ atomic layer deposited after growth of insulator Al2O3. perform magneto-transport measurements and find crossover from weak localization to antilocalization effect with increasing voltage, demonstrates that the Rashba spin-orbit coupling tuned by electrode. The efficiency tuning interaction higher than those obtained for two-dimensional electron gas, as high metal-oxide-semiconductor was previously reported. discussed in line not only conventionally used one-dimensional model but also recently proposed considers effects microscopic band structures materials.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Evolution of microstructure and related optical properties of ZnO grown by atomic layer deposition

A study of transmittance and photoluminescence spectra on the growth of oxygen-rich ultra-thin ZnO films prepared by atomic layer deposition is reported. The structural transition from an amorphous to a polycrystalline state is observed upon increasing the thickness. The unusual behavior of the energy gap with thickness reflected by optical properties is attributed to the improvement of the cry...

متن کامل

Effects of doping and annealing on properties of ZnO films grown by atomic layer deposition

Undoped and Al-doped ZnO films were synthesized by atomic layer deposition at 150°C and then annealed at 350°C in different atmospheres. Effects of doping and annealing on the film growth mode and properties were investigated. The undoped film has strong UV emission and weak Zn interstitial emission. Annealing introduces O vacancies, decreases Zn interstitials, and results in weakening and blue...

متن کامل

Band Offsets and Interfacial Properties of HfAlO Gate Dielectric Grown on InP by Atomic Layer Deposition

X-ray photoelectron spectroscopy and high-resolution transmission electron microscopy have been used to determine interfacial properties of HfO2 and HfAlO gate dielectrics grown on InP by atomic layer deposition. An undesirable interfacial InPxOy layer is easily formed at the HfO2/InP interface, which can severely degrade the electrical performance. However, an abrupt interface can be achieved ...

متن کامل

Studies on ZnO/Si Heterojunction Diode Grown by Atomic Layer Deposition Technique

In this paper studies on Si/ZnO heterojunction diode is presented. In this work Zinc oxide (ZnO) was conformally deposited on Silicon (Si) Wafer by atomic layer deposition (ALD) technique without using a buffer layer. For low-temperature ALD deposition, diethyl zinc (DEZn) and deionized (DI) water were used as the sources for zinc and oxygen respectively. Surface characterization and optical ch...

متن کامل

Enhanced visible photoluminescence from ultrathin ZnO films grown on Si-nanowires by atomic layer deposition.

Bright room temperature visible emission is obtained in heterostructures consisting of approximately 3.5 nm thick ZnO ultrathin films grown on Si-nanowires produced by means of self-masking dry etching in hydrogen-containing plasma. The ZnO films were deposited on Si-nanowires by using atomic layer deposition (ALD) under an ambient temperature of 25 degrees C. The orders of magnitude enhancemen...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Applied Physics Letters

سال: 2021

ISSN: ['1520-8842', '0003-6951', '1077-3118']

DOI: https://doi.org/10.1063/5.0051281