Effects of small amounts of additional elements on stress corrosion cracking of Al-Zn-Mg alloys
نویسندگان
چکیده
منابع مشابه
Tarnish Resistance, Corrosion and Stress Corrosion Cracking of Gold Alloys
Tarnishing, corrosion and stress corrosion cracking (SeC) of gold alloys are related phenomena. They present problems when they occur in gold jewellery, dental gold alloys and electronic devices. They are exploited, however, in the depletion gilding and finishing of gold jewellery; and in the extraction, refining and fire assaying of gold. There is still much that is not known about these pheno...
متن کاملCORROSION BEHAVIOR OF THE Al-Zn-Mg-Cu ALLOYS WITH NICKEL ADDITIONS
In this research, comparative study of corrosion resistance of aluminum based alloys and Al-alloys with nickel have been investigated. Several processes are conducted for the AlZn-Mg-Cu alloys and Al-Zn-Mg-Cu-0.5%Ni alloys were homogenized, aged then retrogressed and reaged; also, alloys were homogenized then the extruded thereafter heat treated. Al-Zn-Mg-Cu alloy and AlZn-Mg-Cu-Ni alloy sample...
متن کاملCORROSION FATIGUE CRACK PROPAGATION AND INHIBITION IN Al-Zn-Mg-Cu VS Al-Cu-Mg/Li ALLOYS
Age-hardenable aluminum alloys used in aerospace structures are susceptible to environment assisted fatigue crack propagation (EFCP), limiting component durability and safety. The objective is to quantitatively understand EFCP and its inhibition for important aerospace alloys: 7075-T651 (Al-Zn-Cu-Mg), C433-T3 (Al-Cu-Mg), and C47A-T86 (AlCu-Li). EFCP is understood through the hydrogen embrittlem...
متن کاملCorrosion Mechanism of Al-zn-in Alloys in Chloride Solutions
The electrochemical behavior of Al-ZnIn alloys was investigated in chloride media by means of potentiodynamic techniques, complemented by Scanning Electron Microscopy (SEM), Energy Dispersive X-Ray Analysis (EDX) and Transmission Electron Microscopy (TEM). The influence of local alkalization produced by previous cathodization was analyzed at potentials more negative than the rest potential. The...
متن کاملthe effects of planning on accuracy and complexity of iranian efl students’ written narrative task performance
this study compared the different effects of form-focused guided planning vs. meaning-focused guided planning on iranian pre-intermediate students’ task performance. the study lasted for three weeks and concentrated on eight english structures. forty five pre-intermediate iranian students were randomly assigned to three groups of guided planning focus-on-form group (gpfg), guided planning focus...
15 صفحه اولذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Japan Institute of Light Metals
سال: 1972
ISSN: 0451-5994
DOI: 10.2464/jilm.22.403