Effects of Sequential Operation with Heat Treatment and Mechanical Milling on Work Hardening for Superalloy GH4169
نویسندگان
چکیده
Engineering components are usually manufactured with sequential production processes. Work hardening due to previous processes affects the machinability of workpiece in subsequent operations. In this research, surface work a by two heat treatment/milling (HT + M) and milling/heat treatment (M HT) superalloy GH4169 was investigated. First, microstructure characteristics, including plastic deformation grain size machined processed processes, were quantitatively presented. Then, microhardness on its cross-section measured analyzed. Finally, calculation model considering twin boundary proposed. Here, we also present evolution principle It found that degree HT M machining 179%, whereas only 101%. The research results can be applied optimized selection process sequence for manufacturing GH4169.
منابع مشابه
Investigation into Grindability of Gh4169 Superalloy and Effects of Grinding Parameters on the Surface Integrity
GH4169, a nickel-base heat-resistant alloy, usually has outstanding high-temperature strength, excellent thermal stability and good wear resistance. However, it is hard to cut and its machined surface quality and integrity are particularly sensitive to a manufacturing process employed. The study reported in this paper was conducted to initially, review existing research on machining-induced sur...
متن کاملcomparison of zoe and vitapex for canal treatment of necrotic primary teeth
چکیده ندارد.
15 صفحه اولEffect of Overage Hardening Heat Treatment on the Micro Structure and Hardness of Nickel-based Super Alloy Rene-80
Rene-80 nickel-base superalloy as an alloy for production of the jet turbine blades shows high mechanical properties as well as microstructure stability during the high temperature engine operation. In this research, age hardening heat treatment cycle was done on the as-cast Rene-80 superalloy. In the following, microstructure, elemental analysis of phases and macro-hardness of the alloy before...
متن کاملInvestigation of the Heat Treatment Effect on Microstructures and Phases of Inconel 713C Superalloy
The application of Inconel 713C is very vast in different industries such as in automobiles, aircrafts, boilers and turbines. In this paper, Inconel 713C specimens were solutionized at 1000 and 1200 °C for 1 hours in order to study changes in phases and the structure of alloy to modify the γ' phase. The optical and the scanning electron microscopy were used to investigate the structure and the ...
متن کاملthe effects of planning on accuracy and complexity of iranian efl students’ written narrative task performance
this study compared the different effects of form-focused guided planning vs. meaning-focused guided planning on iranian pre-intermediate students’ task performance. the study lasted for three weeks and concentrated on eight english structures. forty five pre-intermediate iranian students were randomly assigned to three groups of guided planning focus-on-form group (gpfg), guided planning focus...
15 صفحه اولذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Metals
سال: 2021
ISSN: ['2075-4701']
DOI: https://doi.org/10.3390/met11091367