Effects of Coating Material and Thermal Aging on Fatigue Strengths of a Ni-Base Superalloy, IN738LC, with Protective Coatings.
نویسندگان
چکیده
منابع مشابه
Effect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy
Effect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy Xingbo Liu a,*, ling Xu a, Ever Barbero a, Wei-Di Cao b, Richard L. Kennedy b a West Virginia University, Morgantown, WV 26506-6106, USA b Allvac, an AT! Technologies Company, Monroe, NC 28111-5030, USA Received 22 October 2006; received in revised form 23 March 2007; accepted 10 May 2007 The effec...
متن کاملFormation Mechanism of Silicon Modified Aluminide Coating on a Ni-Base Superalloy
Formation mechanism of silicon modified aluminide coating applied on a nickel base super alloy IN-738 LC by pack cementation process was the subject of investigation in this research. Study of the microstructure and compositions of the coating was carried out, using optical and scanning electron microscopes, EDS and X-ray diffraction (XRD) techniques. The results showed that due to low partial ...
متن کاملEffects of Rare Earth Elements on Properties of Ni-Base Superalloy Powders and Coatings
NiCrMoY alloy powders were prepared using inert gas atomization by incorporation of rare earth elements, such as Mo, Nb, and Y into Ni60A powders, the coatings were sprayed by oxy-acetylene flame spray and then remelted with high-frequency induction. The morphologies, hollow particle ratio, particle-size distribution, apparent density, flowability, and the oxygen content of the NiCrMoY alloy po...
متن کاملThermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy
A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...
متن کاملEFFECTS OF ALUMINIZING PARAMETERS ON THE MICROSTRUCTURE AND THICKNESS OF PT-ALUMINIDE COATING APPLIED ON A NI-BASE SUPERALLOY, GTD-111
In this research, effects of changes in aluminizing conditions on microstructure of Pt - aluminide coating applied oil a Ni - base superalloy GTD -111, has been studied. A thin layer (i.e.68,#mm ) of Pt was electroplated onto the surface of the .samples, and then they were aluminized by pack cementation technique under various conditions of time, temperature, rate of heating and pack powder com...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Society of Materials Science, Japan
سال: 1998
ISSN: 1880-7488,0514-5163
DOI: 10.2472/jsms.47.1143