Effect of Ta on solidification characteristics and mechanical properties of DZ411 Ni-based superalloy

نویسندگان

چکیده

The effects of Ta content (2.72wt.%, 3.10wt.% and 4.00wt.%) on the solidification characteristics mechanical properties directionally solidified DZ411 Ni-based superalloys were investigated. It is found that Mo decreases with increase in liquid phase after directional solidification, indicating addition can reduce element segregation alloys. primary secondary dendrite arm spacings (PDAS SDAS) alloy Ta, which are consistent models by Hunt Wagner. PDAS SDAS provide enough space for growth tertiary arms, hinders unfavorably oriented dendrites. As a result, facilitates favorably More MC carbides γ–γ’ eutectics formed interdendritic regions, attributed to phase. Furthermore, degree supersaturation W, γ matrix increases thus, promotes formation TCP also microhardness both regions alloy, closer Ta.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Solidification Behavior on Microstructures and Mechanical Properties of Ni-Cr-Fe Superalloy Investment Casting

The effect of solidification behavior on the microstructures and mechanical properties of Ni-Cr-Fe superalloy investment casting is given. Metallographic and image analysis have been used to quantitatively examine the microstructures' evolution. For the parts with the thickness of 3 mm and 24 mm, the volume fraction and maximum equivalent radius of the Laves phase increases from 0.3% to 1.2%, f...

متن کامل

Evaluating the Effect of Ta/W Ratio on Microstructure and Stress Rupture Properties of Ni-Based Single Crystal Superalloy PWA1483

In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...

متن کامل

determination of some physical and mechanical properties red bean

چکیده: در این تحقیق، برخی خواص فیزیکی و مکانیکی لوبیا قرمز به-صورت تابعی از محتوی رطوبت بررسی شد. نتایج نشان داد که رطوبت بر خواص فیزیکی لوبیا قرمز شامل طول، عرض، ضخامت، قطر متوسط هندسی، قطر متوسط حسابی، سطح تصویر شده، حجم، چگالی توده، تخلخل، وزن هزار دانه و زاویه ی استقرار استاتیکی در سطح احتمال 1 درصد اثر معنی داری دارد. به طوری که با افزایش رطوبت از 54/7 به 12 درصد بر پایه خشک طول، عرض، ضخام...

15 صفحه اول

effect of bataine and sulphate supplement on wool and milk characteristics and lambs performance in naine ewes

تعداد 20 رأس میش نژاد نائینی 6+-24 ماهه، با میانگین وزن 2/3-+40 کیلوگرم، همراه با 20 رأس بره های آنها در قالب طرح کاملا تصادفی اثر بتائین و مکمل سولفات بر خصوصیات شیر و پشم و عملکرد بره ها بررسی شد. میش ها بطور تصادفی در چهار تیمار قرار گرفتند. تیمارها عبارت بودند از: 1-گروه شاهد 2-بتائین (05/0 درصد ماده خشک) 3-سولفات (24/0 سولفور درصد ماده خشک 4-بتائین هرماه با سولفات. جیره غذائی طبق nrc با مح...

15 صفحه اول

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: China Foundry

سال: 2023

ISSN: ['1672-6421', '2365-9459']

DOI: https://doi.org/10.1007/s41230-023-2118-2