Effect of Nitrogen on Crevice Corrosion and Pepassivation Behavior of Austenitic Stainless Steel

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Corrosion resistance of austenitic stainless steel in sulphuric acid

The resistance and susceptibility of austenitic stainless steel, Type 304, exposed to strong tetraoxosulphate (VI) acids (2 and 5 M concentrations) contaminated with sodium chloride at ambient temperatures was investigated by gravimetric and metallographic/scanning electron microscopy surface characterization methods. Scanning electron microscope (SEM) was used to examine and characterize the t...

متن کامل

An investigation on the passivation behavior of nitrogen enriched AISI 316L austenitic stainless steel

In the present work the effects of plasma nitridization on the passivation behavior of AISI 316L was investigated. To do this; nitriding treatments were carried out at 420°C for 1, 2, 4 and 16 hours. The phase composition and structure of the nitrided layer were studied by Low Angle X-ray diffraction and Scanning Electron Microscopy. The hardness of samples also was evaluated by Vickers microha...

متن کامل

Inhibition Effect of 2,2’-bipyridyl on the Corrosion of Austenitic Stainless Steel in 0.5M H2SO4

The corrosion inhibition of AISI309 austenitic stainless steel by 2,2'-Bipyridyl in 0.5M H 2 SO 4 at 298K was studied using the mass loss’ method, the potentiodynamic polarization (Tafel), the linear polarization (LRP) and the electrochemical impedance spectroscopy (EIS). The results showed a mixed inhibition mode and an increase in the charge transfer resistance, due to inhibitor molecules’ ad...

متن کامل

Corrosion Behavior of Stainless Steel Clad Rebar

Stainless steel clad rebar (SCR) was investigated because it may become a cost-effective means of controlling corrosion in concrete under very aggressive environments. Sound SCR (316L cladding) resisted corrosion in saturated Ca(OH)2 solution (SCS) with up to 5 wt% chloride. Cladding breaks on SCR induced significant corrosion of exposed underlying CS in SCS with only 1 wt% chloride. A computer...

متن کامل

Sensitization Behavior of Gnaw Austenitic Stainless Steel Joints

The present work has been carried out to study the sensitization behavior of AISI 304L austenitic stainless steel weld, fabricated using GTAW (gas tungsten arc welding process). This weld was subjected to post weld thermal aging (PWTA) treatments lying in the sensitization range, viz. 700 ?C for 30 minutes, 500 minutes and 1000 minutes for studying the influence of carbide precipitation on thei...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Japan Institute of Metals

سال: 2007

ISSN: 1880-6880,0021-4876

DOI: 10.2320/jinstmet.71.570