Effect of Ni Content on Solidification Cracking Susceptibility of Ni-base Superalloy Inconel 706.
نویسندگان
چکیده
منابع مشابه
Effect of Solidification Behavior on Microstructures and Mechanical Properties of Ni-Cr-Fe Superalloy Investment Casting
The effect of solidification behavior on the microstructures and mechanical properties of Ni-Cr-Fe superalloy investment casting is given. Metallographic and image analysis have been used to quantitatively examine the microstructures' evolution. For the parts with the thickness of 3 mm and 24 mm, the volume fraction and maximum equivalent radius of the Laves phase increases from 0.3% to 1.2%, f...
متن کاملCreep Crack Growth Simulation of Ni-base Superalloy
The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...
متن کاملEffect of pre-exposure on crack initiation life of a directionally solidified Ni-base superalloy
Article history: Received 6 February 2008 Received in revised form 1 July 2008 Accepted 24 July 2008 Available online 5 August 2008
متن کاملThermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy
A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...
متن کاملEffect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy
Effect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy Xingbo Liu a,*, ling Xu a, Ever Barbero a, Wei-Di Cao b, Richard L. Kennedy b a West Virginia University, Morgantown, WV 26506-6106, USA b Allvac, an AT! Technologies Company, Monroe, NC 28111-5030, USA Received 22 October 2006; received in revised form 23 March 2007; accepted 10 May 2007 The effec...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY
سال: 1998
ISSN: 0288-4771
DOI: 10.2207/qjjws.16.365