Effect of Nanosilica Incorporation on Flexural Strength, Shear Bond Strength, and Color of Veneering Porcelain after Thermocycling
نویسندگان
چکیده
AIM: The focus of this research was to see how silica nanoparticles changed veneering porcelain over a zirconia core affected flexure strength, shear bond and color. METHODS: A total number 30 veneer samples were constructed classified according modification into two groups: Group 1 (control group) without any (n = 15) 2 (modified modified by 15). Silica added the powder at rate 5% weight. manually crushed for about 10 min using pestle mortar then mixed combined with moldings liquid make paste. After thermal cycling, each group examined flexural color measurement 5). Universal testing equipment used determine strength. shift measured spectrophotometer. RESULTS: Flexural strength levels in (280.9 ± 29.85 Mpa) substantially higher than control (431.78 22.73 Mpa). Shear values (34.31 5.6) significantly (26.97 4.03). Color change within clinical acceptable range (1.71 0.32). CONCLUSIONS: addition improved as well as, limits.
منابع مشابه
Shear bond strength of veneering porcelain to porous zirconia.
In this study, two types of porous zirconia and dense zirconia were used. The flexural strength of non-layered zirconia specimens and those of the layered zirconia specimens with veneering porcelain were examined. Furthermore, the shear bond strength of veneering porcelain to zirconia was examined. The flexural strength of the non-layered specimens was 1,220 MPa for dense zirconia and 220 to 30...
متن کاملShear Bond Strength of Porcelain Veneering to Nickel-Chromium, Chromium-Cobalt, Zirconia and Lithium Disilicate
Background and Aim: High chipping rates of the veneering porcelain in zirconia ce-ramic restorations have been reported in many clinical studies. However, information on the bonding behavior of veneering porcelain to zirconia and lithium disilicate frameworks is limited. The purpose of this study was to evaluate the bond-ing strength of porcelain veneering to zirconia, lithium disilicate, nicke...
متن کاملEffect of cooling rate on shear bond strength of veneering porcelain to a zirconia ceramic material.
The purpose of the present study was to evaluate the effect of cooling rates after firing procedures of veneering porcelain on shear bond strength between veneering porcelain and a zirconium dioxide (zirconia; ZrO₂) ceramic material. A total of 48 ZrO₂ disks were divided equally into three groups. Two veneering porcelains that are recommended for ZrO₂ material - Cerabien ZR (CZR), IPS e.max Cer...
متن کاملINFLUENCE OF SURFACE TREATMENT ON VENEERING PORCELAIN SHEAR BOND STRENGTH TO ZIRCONIA AFTER CYCLIC LOADING by
.................................................................................... 66
متن کاملShear bond strength between an indirect composite veneering material and zirconia ceramics after thermocycling.
The present study evaluated the shear bond strength between an indirect composite material and zirconium dioxide (zirconia) ceramics after thermocycling. A total of 80 zirconia (Katana) discs were divided into five groups and primed with one of following agents: All Bond 2 Primer B (ABB), Alloy Primer (ALP), AZ Primer (AZP), Estenia Opaque Primer (EOP), and Porcelain Liner M Liquid A (PLA). An ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Open Access Macedonian Journal of Medical Sciences
سال: 2022
ISSN: ['1857-9655']
DOI: https://doi.org/10.3889/oamjms.2022.10390