Effect of Microstructure on the Localized Corrosion and Stress Corrosion Behaviours of Plasma-Electrolytic-Oxidation-Treated AA7075 Aluminum Alloy Forging in 3.5 wt. %NaCl Solution

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Plasma Electrolytic Oxidation Process as a Pretreatment on Corrosion Resistance of Polymeric Coatings Applied on Mg Alloy

In this study, Plasma Electrolytic Oxidation (PEO) at three frequencies of 500, 1000 and 3000 Hz was applied on Mg surface and the effect of PEO surface preparation on protective behavior of three types of epoxy, fusion bond epoxy (FBE) and polyurethane coatings was investigated. The microstructural and protective properties of PEO coatings were studied by SEM, potentiodynamic polarization and ...

متن کامل

Effect of Plasma Electrolytic Oxidation Process as a Pretreatment on Corrosion Resistance of Polymeric Coatings Applied on Mg Alloy

In this study, Plasma Electrolytic Oxidation (PEO) at three frequencies of 500, 1000 and 3000 Hz was applied on Mg surface and the effect of PEO surface preparation on protective behavior of three types of epoxy, fusion bond epoxy (FBE) and polyurethane coatings was investigated. The microstructural and protective properties of PEO coatings were studied by SEM, potentiodynamic polarization and ...

متن کامل

plasma electrolytic oxidation of 2024-t3 aluminum alloy and study of its corrosion resistance and tribological behavior

in this study, plasma electrolytic oxidation of 2024-t3 aluminum alloy was investigated. the electrolyte used in this investigation was an alkaline solution containing additives of silicate, phosphate, potassium hydroxide and glycerin. a conventional dc power source with a low applied voltage was employed. corrosion resistance of the oxide layer was investigated by means of tafel plots and elec...

متن کامل

Corrosion behavior and cytocompatibility of fluoride-incorporated plasma electrolytic oxidation coating on biodegradable AZ31 alloy

Fluoride-incorporated plasma electrolytic oxidation (PEO) coating was fabricated on biodegradable AZ31 alloy. The surface morphologies and phases were investigated by scanning electron microscopy and X-ray diffraction. The effect of fluoride incorporation in coatings on corrosion behaviour was investigated in simulated body fluid and in vitro cytocompatibility of the coatings was also studied b...

متن کامل

Effect of Procedure Time on Microstructure and Corrosion Behavior of ZrTiO4/ZrO2 Nanocomposite Coatings by Plasma Electrolytic Oxidation (PEO) Applied on the Ti-6Al-4V Substrate

In this research, the effect of PEO procedure time on the distinct properties of coatings such as morphology, chemical composition, roughness and corrosion has been studied. A scanning electron microscopy equipped with an energy dispersive spectroscopy was used to study the microstructure of the coatings. In addition, x-ray diffraction (XRD) and roughness meter were used to evaluate the chemica...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International Journal of Corrosion

سال: 2012

ISSN: 1687-9325,1687-9333

DOI: 10.1155/2012/823967