Effect of Microstructure and Corrosive Environments on Stress-Corrosion Cracking in Al-Zn-Mg Alloys
نویسندگان
چکیده
منابع مشابه
Effect of Homogenization on Microstructure Characteristics, Corrosion and Biocompatibility of Mg-Zn-Mn-xCa Alloys
The corrosion behaviors of Mg-2Zn-0.2Mn-xCa (denoted as MZM-xCa alloys) in homogenization state have been investigated by immersion test and electrochemical techniques in a simulated physiological condition. The microstructure features were characterized using scanning electron microscopy (SEM), X-ray diffraction (XRD), transmission electron microscopy (TEM) and electron probe microanalysis (EP...
متن کاملMicrostructure of Al-Zn and Zn-Al Alloys*
The change of microstructure of the title alloys with concentration, temperature and applied thermal treatment was studied in situ by XRD. The alloys, having the Zn atomic fraction, x(Zn), from 0.03 to 0.62, were subjected to: (i) rapid quenching from a temperature, Tt, higher than the solid-solution temperature, Tss, in water at RT (samples WQ); (ii) slow cooling from Tt to RT (samples SC). Th...
متن کاملEffect of Microstructure Factors on Stress Corrosion Behavior of Mg-xSn Alloys (x=2, 5, 8mass%)
The effect of microstructure on the stress corrosion behavior of Mg–Sn alloys was investigated using a bent-beam method. The effects of an Mg2Sn phase and Sn in the matrix on stress corrosion were investigated. Mg2Sn phase mainly formed at the grain boundary. The volume fraction of the Mg2Sn phase increased with increasing Sn content, and the morphology of Mg2Sn changed from spherical to a semi...
متن کاملTarnish Resistance, Corrosion and Stress Corrosion Cracking of Gold Alloys
Tarnishing, corrosion and stress corrosion cracking (SeC) of gold alloys are related phenomena. They present problems when they occur in gold jewellery, dental gold alloys and electronic devices. They are exploited, however, in the depletion gilding and finishing of gold jewellery; and in the extraction, refining and fire assaying of gold. There is still much that is not known about these pheno...
متن کاملCORROSION FATIGUE CRACK PROPAGATION AND INHIBITION IN Al-Zn-Mg-Cu VS Al-Cu-Mg/Li ALLOYS
Age-hardenable aluminum alloys used in aerospace structures are susceptible to environment assisted fatigue crack propagation (EFCP), limiting component durability and safety. The objective is to quantitatively understand EFCP and its inhibition for important aerospace alloys: 7075-T651 (Al-Zn-Cu-Mg), C433-T3 (Al-Cu-Mg), and C47A-T86 (AlCu-Li). EFCP is understood through the hydrogen embrittlem...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Institute of Metals and Materials
سال: 1979
ISSN: 0021-4876,1880-6880
DOI: 10.2320/jinstmet1952.43.7_671