The study of fatigue behaviors for nickel-base superalloys is very significant because fatigue damage results in serious consequences. In this paper, two kinds of heat treatment procedures (Pro.I and Pro.II) were taken to investigate the effect of heat treatment on microstructures and fatigue behaviors of a nickel-base superalloy. Fatigue behaviors were studied through total strain controlled m...
متن کاملEffect of Heat Treatment Process on the Fatigue Behavior of AISI 1060 Steel
This experimental study investigated the effects of quenching and tempering heat treatment on fatigue behavior and also tempering temperature and time holding of AISI 1060 steel. At first, the specimens were austenitized at 800˚C for 1 hour, and then were quenched in the water bath of 25˚C temperature. After that, tempering process was done at the temperature of 250˚C, 450˚C and 650˚C for 1 and...
متن کاملEffect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy
Effect of thermal treatment on the fatigue crack propagation behavior of a new Ni-base superalloy Xingbo Liu a,*, ling Xu a, Ever Barbero a, Wei-Di Cao b, Richard L. Kennedy b a West Virginia University, Morgantown, WV 26506-6106, USA b Allvac, an AT! Technologies Company, Monroe, NC 28111-5030, USA Received 22 October 2006; received in revised form 23 March 2007; accepted 10 May 2007 The effec...
متن کاملFatigue Behavior and Life Prediction Model of a Nickel-Base Superalloy under Different Strain Conditions
The fatigue behavior of a nickel-base superalloy was investigated under total strain-controlled mode at high temperature. The fatigue life, cyclic stress response behavior and hysteresis loop of the superalloy were investigated under isothermal low cycle fatigue (LCF) conditions. The superalloy exhibited cyclic hardening and softening behaviors during the process of fatigue loading. The hystere...