Effect of heat input on joint performance in 6061 aluminum alloy friction welding.
نویسندگان
چکیده
منابع مشابه
Welding Aluminum Alloy 6061 with Opposing Dual Torch Gtaw Process
Cracking is a major concern in welding aluminum alloys. Although weld solidification cracks can be eliminated through addition of filler alloy, the additives modify the alloy or base-metal constituents and may not always be desirable. High-energy beam processes, such as electron-beam welding, that result in minimal heat input reduce crack sensitivity, but their high cost limits their applicatio...
متن کاملEffect of Heat Input on Microstructure and Mechanical Properties in Friction Stir Welding of HSLA-60
High-strength low alloy steels are a class of steels used in applications that require high strength and good weldability, including ship hulls, gas pipelines and oil industry. One way to build parts is fusion welding that create areas with a large grain size in the heat-affected zone and increased susceptibility to hydrogen cracking. One way to solve this problem is to use solid state friction...
متن کاملFriction stir welding of dissimilar joint of aluminum alloy 5083 and commercially pure titanium
In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important ...
متن کاملEffect of Heat Input on Microstructure and Mechanical Properties in Friction Stir Welding of HSLA-60
High-strength low alloy steels are a class of steels used in applications that require high strength and good weldability, including ship hulls, gas pipelines and oil industry. One way to build parts is fusion welding that create areas with a large grain size in the heat-affected zone and increased susceptibility to hydrogen cracking. One way to solve this problem is to use solid state friction...
متن کاملFriction stir welding of dissimilar joint of aluminum alloy 5083 and commercially pure titanium
In this study, commercially pure titanium and aluminum alloy 5083 in connection rotational speed of 1120 rpm and a feed rate of 50 mm per minute for butt welding by friction stir welding has been successfully completed. Micro-structure, hardness and tensile test was conducted on the connection. Welding area is a composite of aluminum and titanium particles that the particles plays an important ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Japan Institute of Light Metals
سال: 2000
ISSN: 0451-5994,1880-8018
DOI: 10.2464/jilm.50.505