Effect of Different Aging Times on Sn-Ag-Cu Solder Alloy
نویسندگان
چکیده
منابع مشابه
Mechanical Properties and Solder Joint Reliability of Low-Melting Sn-Bi-Cu Lead Free Solder Alloy
The influence of alloy composition of lowmelting Sn-Bi-Cu lead-free solder alloys on mechanical properties and solder joint reliabilities were investigated. The mechanically optimum alloy composition is Sn-40Bi-0.1Cu (mass%). The addition of 40mass%Bi improves the ductility and restrains the fillet-lifting, which are problems of lead-free solders with Bi. The addition of copper improves both th...
متن کاملHigh-Reliability Low-Ag-Content Sn-Ag-Cu Solder Joints for Electronics Applications
Sn-Ag-Cu (SAC) alloy is currently recognized as the standard lead-free solder alloy for packaging of interconnects in the electronics industry, and highAg-content SAC alloys are the most popular choice. However, this choice has been encumbered by the fragility of the solder joints that has been observed in drop testing as well as the high cost of the Ag itself. Therefore, low-Ag-content SAC all...
متن کاملThe Anomalous Microstructural , Tensile and Aging Response of Thin Cast Sn 3 . 9 Ag 0 . 6 Cu Lead Free Solder
-In this study bulk and thin cast samples were produced with an identical Sn3.9Ag0.6Cu composition. The thin cast material exhibited a much finer as-quenched microstructure than the bulk material with the IMC phase restricted to a thin network. Both the bulk and thin cast materials continually softened during room temperature aging, while both materials initially softened and then subsequently ...
متن کاملInfluence of nanoparticle addition on the formation and growth of intermetallic compounds (IMCs) in Cu/Sn–Ag–Cu/Cu solder joint during different thermal conditions
Nanocomposite lead-free solders are gaining prominence as replacements for conventional lead-free solders such as Sn-Ag-Cu solder in the electronic packaging industry. They are fabricated by adding nanoparticles such as metallic and ceramic particles into conventional lead-free solder. It is reported that the addition of such nanoparticles could strengthen the solder matrix, refine the intermet...
متن کاملMechanical Characterization of Lead-Free Sn-Ag-Cu Solder Joints by High-Temperature Nanoindentation
The reliability of Pb-free solder joints is controlled by their microstructural constituents. Therefore, knowledge of the solder microconstituents' mechanical properties as a function of temperature is required. Sn-Ag-Cu lead-free solder alloy contains three phases: a Sn-rich phase, and the intermetallic compounds (IMCs) CueSn5 and Ag3Sn. Typically, the Sn-rich phase is surrounded by a eutectic...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Transactions on Electrical and Electronic Materials
سال: 2015
ISSN: 1229-7607
DOI: 10.4313/teem.2015.16.3.112