Effect of Base Metal Grain Boundary on TLP-Bonding Phenomena of CMSX-2. Transient Liquid Phase Bonding of Ni-Base Single Crystal Superalloy. (Report 3).

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of bonding time on microstructure and mechanical properties during TLP bonding of nickel-base superalloys Hastelloy C276 and Stainless Steel AISI316

Joining of Hastelloy C276 nickel-base superalloy to AISI316 Stainless Steel using BNi-2 interlayer performed by transient liquid phase process (TLP) at 1150°C for 5 and 30 minutes. Bonding microstructure was studied using an Optical microscope and a scanning electron microscope (SEM). Vickers hardness test and shear strength test have been used to evaluate the mechanical properties. Microstruct...

متن کامل

Effect of bonding time on microstructure and mechanical properties during TLP bonding of nickel-base superalloys Hastelloy C276 and Stainless Steel AISI316

Joining of Hastelloy C276 nickel-base superalloy to AISI316 Stainless Steel using BNi-2 interlayer performed by transient liquid phase process (TLP) at 1150°C for 5 and 30 minutes. Bonding microstructure was studied using an Optical microscope and a scanning electron microscope (SEM). Vickers hardness test and shear strength test have been used to evaluate the mechanical properties. Microstruct...

متن کامل

The effect of bonding temperature on the characteristics of TLP bonded joints in AISI 2205/BNi-3/AISI 2205 assembly

In the present study, the transient liquid phase bonding of AISI 2205 dual phase stainless steel with amorphous BNi-3 interlayer was carried out. Based on the initial experimental and analytical studies, the parameters of temperature and bonding time were determined. In order to investigate the effect of bonding temperature on the microstructural changes of the joint, bonding was performed in t...

متن کامل

The effect of bonding temperature on the characteristics of TLP bonded joints in AISI 2205/BNi-3/AISI 2205 assembly

In the present study, the transient liquid phase bonding of AISI 2205 dual phase stainless steel with amorphous BNi-3 interlayer was carried out. Based on the initial experimental and analytical studies, the parameters of temperature and bonding time were determined. In order to investigate the effect of bonding temperature on the microstructural changes of the joint, bonding was performed in t...

متن کامل

On the microstrctral and machanical properties of similar TLP bonding of Inconel 600 superalloy sheet

In this study, microstructural evaluation and mechanical properties of similar TLP bonded of Inconel 600 by using of BNi-2 interlayer were investigated. The bonding tests were carried out at 1050°C and 1100°C for 5-45 min which homogenization treatment was performed on the best of the bonded samples. Results showed that Ni-B eutectic compound was formed in the a-thermally solidification zone (A...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY

سال: 1997

ISSN: 0288-4771

DOI: 10.2207/qjjws.15.321