Influences of Sample Preparation on Nanoindentation Behavior of a Zr-Based Bulk Metallic Glass
Influences of two different sample preparation methods, mechanical polishing and plunge cutting, on nanoindentation behavior of a Zr-based bulk metallic glass were studied. Mechanical polishing suppresses the serrated flow but promotes the creep. In contrast, plunge cutting promotes the serrated flow but suppresses the creep. However, hardness and elastic modulus obtained from these two methods...
متن کاملEffects of annealing and specimen geometry on dynamic compression of a Zr-based bulk metallic glass
High strain-rate compression experiments were performed with a split-Hopkinson pressure bar (SHPB) at 500–4000/s on cylindrical samples of a Zr-based bulk metallic glass (LM-1) in both the fully amorphous and annealed conditions. The effects of changes to the specimen geometry (i.e., L/D ratio) and the material heat treatment [i.e., annealing versus amorphous (as-received)], on the peak stress,...
متن کاملRate dependence of serrated flow during nanoindentation of a bulk metallic glass
Plastic deformation of Pd–40Ni–20P bulk metallic glass (BMG) was investigated by instrumented nanoindentation experiments over a broad range of indentation strain rates. At low rates, the load–displacement curves during indentation exhibited numerous serrations or pop-ins, but these serrations became less prominent as the indentation rate was increased. Using the tip velocity during pop-in as a...
متن کاملDuctile bulk metallic glass.
We report on experimental evidence of pronounced global plasticity measured in monolithic Pt57.5Cu14.7Ni5.3P22.5 bulk metallic glass under both bending and unconfined compression loading conditions. A plastic strain of 20% is measured, never before seen in metallic glasses. Also, permanent deformation and a strain exceeding 3% before failure is observed during bending of 4 mm thick samples. To ...
متن کاملBulk metallic glass matrix composites
Composites with a bulk metallic glass matrix were synthesized and characterized. This was made possible by the recent development of bulk metallic glasses that exhibit high resistance to crystallization in the undercooled liquid state. In this letter, experimental methods for processing metallic glass composites are introduced. Three different bulk metallic glass forming alloys were used as the...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Physical Review B
سال: 2017
ISSN: 2469-9950,2469-9969
DOI: 10.1103/physrevb.96.134117