Effect of Acidizing Process on the Stress Corrosion Cracking of HP-13Cr Stainless Steel in the Ultra-depth Well Environment
نویسندگان
چکیده
The effect of acidizing process on the stress corrosion cracking HP-13Cr stainless steel in ultra-depth well environment was studied by slow strain rate test, electrochemical measurement, microstructure observation, and finite element modeling. results indicated that significantly increased susceptibility induced fracture mode to brittle characteristic high temperature CO 2 pressure environment. also with increase pressure. There were dense defects including pits cracks section from transverse view. After process, under tensile condition, increasing roughness will cause concentration promote local anodic dissolution, which induces initiation cracking.
منابع مشابه
the effect of taftan pozzolan on the compressive strength of concrete in the environmental conditions of oman sea (chabahar port)
cement is an essential ingredient in the concrete buildings. for production of cement considerable amount of fossil fuel and electrical energy is consumed. on the other hand for generating one tone of portland cement, nearly one ton of carbon dioxide is released. it shows that 7 percent of the total released carbon dioxide in the world relates to the cement industry. considering ecological issu...
the washback effect of discretepoint vs. integrative tests on the retention of content in knowledge tests
در این پایان نامه تاثیر دو نوع تست جزیی نگر و کلی نگر بر به یادسپاری محتوا ارزیابی شده که نتایج نشان دهندهکارایی تستهای کلی نگر بیشتر از سایر آزمونها است
15 صفحه اولthe effect of e-64 on the developmental competence of sheep cocs during in vitro maturation
in the present study, the effect of e-64 at different concentrations (0.5, 1, 5 and 10 µm) added to (1) the ivm medium on oocyte nuclear maturation and developmental competence of ovine oocytes, and (2) to the ivc medium on embryonic development of ovine embryos were investigated.
the effect of learning strategies on the speaking ability of iranian students in the context of language institutes
the effect of learning strategies on the speaking ability of iranian students in the context of language institutes abstract language learning strategies are of the most important factors that help language learners to learn a foreign language and how they can deal with the four language skills specifically speaking skill effectively. acknowledging the great impact of learning strategies...
the effect of authentic listening materials on the listening proficiency of efl learners in the intermediate level
having conducted the experiment and analysed the data, the researcher computed the groups mean scores and variances for the test relating to the research question. as the final atep, a t-test was conodonted for the hypothesis. as noted earlier, the significance level was determined at .05 and .01 respectively. the observed t-value was higher than the critical t-value at. 5 and .01 levels. conse...
15 صفحه اولذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Frontiers in Materials
سال: 2021
ISSN: ['2296-8016']
DOI: https://doi.org/10.3389/fmats.2021.732931