Ductile iron with nodular and compact graphite as a rational alternative to malleable cast iron
نویسندگان
چکیده
There is a need for cast irons with combined combination of properties in modern conditions. Such can be provided by ductile iron nodular and vermicular graphite, which essentially hybrid terms microstructure. The article found that graphite its mechanical rational alternative to malleable iron, namely the grade KCh45-6 (GOST 1215-79). Also, ratio nodular/vermicular (70…95/5…30%) was determined, provides data characteristics. Differences pearlite/ferrite hardness are shown, providing KCh45-6.
منابع مشابه
Fatigue Performance of Forged Steel and Ductile Cast Iron Crankshafts
Fatigue is the primary cause of failure of crankshafts in internal combustion engines. The cyclic loading conditions and the stress concentrations in the crank pin fillets are unavoidable, and can result in fatigue failure. The objectives of this study were to compare the fatigue behavior of forged steel and ductile iron crankshafts from a one-cylinder engine as well as to determine if the fati...
متن کاملNDT of Ductile Cast Iron from Nuclear Waste Storage Canisters
The concept for geological disposal of nuclear waste and spent nuclear fuel relies on a multi-barrier system with the copper/cast iron canister as the first barrier. The canister is designed to retain its integrity for at least 100000 years, which means that future glaciations need to be considered. A thick ice block together with hydrostatic pressure from groundwater would produce hydrostatic ...
متن کاملPearlitic ductile cast iron: damaging micromechanisms at crack tip
Ductile cast irons (DCIs) are characterized by a wide range of mechanical properties, mainly depending on microstructural factors, as matrix microstructure (characterized by phases volume fraction, grains size and grain distribution), graphite nodules (characterized by size, shape, density and distribution) and defects presence (e.g., porosity, inclusions, etc.). Versatility and higher performa...
متن کاملFailure Analysis of a Four Cylinder Diesel Engine Crankshaft Made From Nodular Cast Iron
The premature breakage in some four cylinder diesel engine crankshafts was reported. All crankshafts were failed from the same region. Failures had occurred in the first crankpin, the nearest crankpin to the flywheel. Dynamic analysis and finite element modelling were carried out to determine the state of stress in the crankshaft. FEM results revealed that the first crankpin fillet is the most ...
متن کاملLiterature search - Deteriorated Graphite Structures on Cast Iron Skins
The fatigue strength offerritic ductile iron, Grade EN-GJS-400-18U-LT. was determined for large section castings measuring 4 by 24 by 24 inches. Fatigue testing was conducted in bending fatigue in order to determine the influence of surface conditions on fatigue strength. Test specimens with various surface conditions were evaluated, including notched and un-notched specimens, as well as those ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: E3S web of conferences
سال: 2023
ISSN: ['2555-0403', '2267-1242']
DOI: https://doi.org/10.1051/e3sconf/202338902019