Dissolution of Glass–Ceramic Scaffolds of Bioactive Glasses 45S5 and S53P4

نویسندگان

چکیده

Abstract Although the initial in vitro dissolution of bioactive glasses (BAG) is well characterized, long-term behaviour crystallized BAG scaffolds a continuous fluid flow incompletely understood. A detailed understanding vital for predicting their clinical applications. Here, we explored and reaction mechanisms partly crystalline glass–ceramic based on S53P4 45S5 using flow-through method Tris-buffer (Tris) simulated body (SBF) up to 21 days. Granules parent were used as references. The main phase both was sodium-calcium-silicate. scaffolds’ suggested that sodium-calcium-silicate crystals dissolved incongruently yield hydrous silica. silica then provided abundant nucleation sites hydroxyapatite precipitation, resulting fine-grained structures. When exposed Tris, almost completely within test period, leaving only highly porous remnant phases. For scaffolds, calcium phosphate layers formed surfaces effectively slowed SBF. In contrast, this effect less apparent specimens.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Elastic Properties of substituted 45S5 Bioactive Glasses and Glass - Ceramics

CuO, Fe2O3, MnO2 and ZnO substituted 45S5 bioactive glasses were prepared. Glass derived Bioactive Glass ceramics were obtained through controlled crystallization of bioactive glasses. The formed crystalline phases in bioactive glass ceramics were identified using X ray diffraction (XRD) analysis. Density and ultrasonic wave velocities of bioactive glasses and glass ceramics were measured and u...

متن کامل

Fabrication of 45s5 Bioactive Glass-polycaprolactone Composite Scaffolds

Tissue engineering is a multi-disciplinary field, which aims to apply innovative biomaterials to replace or restore ill or damaged tissues of the human body, such as skin and bones. In particular, porous scaffolds are used as temporary 3D templates to support cell attachment and proliferation during the spontaneous regeneration of natural tissues and this approach is particularly promising for ...

متن کامل

In Vitro Bioactivity and Physical - Mechanical Properties of Fe2O3 substituted 45S5 Bioactive Glasses and Glass - ceramics

Abstract — Fe2O3 substituted 45S5 bioactive glasses were prepared. Glass derived Bioactive Glass ceramics were obtained through controlled crystallization of bioactive glasses. Nucleation and crystallization regimes were determined by the parameters obtained from differential thermal analysis (DTA) of bioactive glasses. The formed crystalline phases in bioactive glass ceramics were identified u...

متن کامل

Preparation and characterization of fluorapatite-bioactive glass S53P4 nanocomposite

This research has been done to study characteristic and biocompatible evaluation of a nano-biocompositeceramic with the bioglass (BG) as a first phase. In this regard, synthesis of S53P4 (53% SiO2, 4% P2O5,23% Na2O and 20% CaO) bioglass has been considered as the first phase and flourapatite (FA) consideredas the second phase. Afterwards, nanocomposite with the base of S53P4 b...

متن کامل

Bioactive Glasses: From Parent 45S5 Composition to Scaffold-Assisted Tissue-Healing Therapies

Nowadays, bioactive glasses (BGs) are mainly used to improve and support the healing process of osseous defects deriving from traumatic events, tumor removal, congenital pathologies, implant revisions, or infections. In the past, several approaches have been proposed in the replacement of extensive bone defects, each one with its own advantages and drawbacks. As a result, the need for synthetic...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Biomedical Materials & Devices

سال: 2023

ISSN: ['2731-4812', '2731-4820']

DOI: https://doi.org/10.1007/s44174-022-00059-4