Discharge Characteristics in Electrochemical Discharge Machining of Ceramic-coated Ni-superalloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Electrical Discharge Machining of Ceramic/semiconductor/metal Nanocomposites

Electroconductive, homogeneous and dense ceramic/semiconductor/metal nanocomposites were obtained by hot press and subsequently machined by wire Electrical Discharge Machining (EDM). The addition of semiconductor and metal phases to a highperformance ceramic material produces nanocomposites which preserve the excellent mechanical properties of the ceramic/metal material while reaching the elect...

متن کامل

Wireless Sensing of Discharge Characteristics for Quality Control in Batch Mode Micro-electro-discharge Machining

Wireless signals are inherently generated during the spark discharges of micro-electro-discharge machining (μEDM). This work harnesses signals between 300-750 MHz for the monitoring of batch mode machining quality. In particular, the wireless spectra are used to sense incipient, debris-dominated machining that can be destructive to both the tool and the workpiece. Planar stainless steel (316L) ...

متن کامل

Charge/discharge and Electrochemical Characteristics of Secondary Lithium/pyrite Battery

Iron disulfide (FeS2) is attractive as a positive electrode material in lithium batteries because of its low material cost, environmental non-toxicity, and high specific energy density. Furthermore, natural pyrite is a secondary product of the mining extraction of coal. For these reasons, natural and synthetic pyrites have been proposed as active cathode materials in secondary lithium batteries...

متن کامل

Optimization of Machining Parametric Study on Electrical Discharge Machining

Abstract—Productivity and quality are two important aspects that have become great concerns in today’s competitive global market. Every production/manufacturing unit mainly focuses on these areas in relation to the process, as well as the product developed. The electrical discharge machining (EDM) process, even now it is an experience process, wherein the selected parameters are still often far...

متن کامل

Influence of electrical discharge machining on sliding friction and wear of WC–Ni cemented carbide

Tribological characteristics of fine-grained WC–8 wt%Ni with different surface finishing conditions corresponding to sequential wire electrical discharge machining (wire-EDM) or grinding were investigated by performing dry reciprocating sliding experiments on TE77 pin-on-plate equipment with WC–6 wt%Co as mating material. Surface finishes and wear surfaces were characterized using surface topog...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Procedia CIRP

سال: 2020

ISSN: 2212-8271

DOI: 10.1016/j.procir.2020.02.307