Sulfur particles with a conductive polymer coating of poly(3,4-ethylene dioxythiophene) “PEDOT” were prepared by dielectric barrier discharge (DBD) plasma technology under atmospheric conditions (low temperature, ambient pressure). We report solvent-free, low-cost, low-energy-consumption, safe, and low-risk process to make the material development production compatible for sustainable technologies. Different protocols developed produce PEDOT-coated sulfur powders electrical conductivity in range 10–8–10–5 S/cm. The raw powder (used as reference) (low-, optimum-, high-) used assemble lithium–sulfur (Li–S) cells high loading ?4.5 mg/cm2. Long-term galvanostatic cycling at C/10 100 cycles showed that capacity fade was mitigated ?30% containing optimum-PEDOT-coated comparison reference Li–S sulfur. Rate capability, cyclic voltammetry, electrochemical impedance analyzes confirmed improved behavior an active batteries. highest reproducibility their properties. A wide variety bulk surface characterization methods including analysis, X-ray diffraction (XRD), scanning electron microscopy (SEM), Raman spectroscopy, photoelectron spectroscopy (XPS), NMR explain chemical features superior using material. Moreover, postmortem [SEM Brunauer–Emmett–Teller (BET)] uncoated coated samples allowed us exclude any significant effect electrode scale even after 70 cycles.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Capacity Fade Analysis of Sulfur Cathodes in Lithium–Sulfur Batteries

Rechargeable lithium-sulfur (Li-S) batteries are receiving ever-increasing attention due to their high theoretical energy density and inexpensive raw sulfur materials. However, their rapid capacity fade has been one of the key barriers for their further improvement. It is well accepted that the major degradation mechanisms of S-cathodes include low electrical conductivity of S and sulfides, pre...

متن کامل

Surface Decontamination by Dielectric Barrier Discharge Plasma

Background: Dielectric barrier discharge (DBD), a source of non-thermal plasma, is used in surface decontamination. Objective: To study the effect of DBD plasma treatment, we evaluated the effect of plasma exposure time on inactivation of Bacillus subtilis. Results: Applying the DBD plasma to the culture of B. subtilis caused complete sterilization of the surface without any thermal effects. In...

متن کامل

surface decontamination by dielectric barrier discharge plasma

background: dielectric barrier discharge (dbd), a source of non-thermal plasma, is used in surface decontamination. objective: to study the effect of dbd plasma treatment, we evaluated the effect of plasma exposure time on inactivation of bacillus subtilis. results: applying the dbd plasma to the culture of b. subtilis caused complete sterilization of the surface without any thermal effects. in...

متن کامل

Dielectric Barrier Discharge (DBD) Plasma Assisted Synthesis of Ag₂O Nanomaterials and Ag₂O/RuO₂ Nanocomposites.

Silver oxide, ruthenium oxide nanomaterials and its composites are widely used in a variety of applications. Plasma-mediated synthesis is one of the emerging technologies to prepare nanomaterials with desired physicochemical properties. In this study, dielectric barrier discharge (DBD) plasma was used to synthesize Ag₂O and Ag₂O/RuO₂ nanocomposite materials. The prepared materials showed good c...

متن کامل

Dielectric Barrier Discharge (DBD) Plasma Assisted Synthesis of Ag2O Nanomaterials and Ag2O/RuO2 Nanocomposites

Figure S1a,b show the optical and field emission scanning electron microscope (FESEM) images of the RuO2 NMs. The nanomaterials exhibited nanosheet morphology with length >1 μm and the width <100 nm. The X-ray diffraction (XRD) spectrum (Figure S1c) showed the prominent peaks at the diffraction angle (2θ) 28.00, 34.93, 39.64 and 54.00, representing (110), (101), (200) and (211) set of latti...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: ACS Applied Materials & Interfaces

سال: 2021

ISSN: ['1944-8244', '1944-8252']

DOI: https://doi.org/10.1021/acsami.1c04069