Die-Casting Defect Prediction and Diagnosis System using Process Condition Data

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Die-Casting Process Modeling Using Neural Networks

This chapter presents the application of a neural network to the industrial process modeling of high-pressure die casting (HPDC). The large number of interand intradependent process parameters makes it difficult to obtain an accurate physical model of the HPDC process that is paramount to understanding the effects of process parameters on casting defects such as porosity. The first stage of the...

متن کامل

Optimization of Aluminium Die Casting Process Using Artificial Neural Network

In the present paper, optimization of process parameters of an aluminium die casting operation is discussed. The quality problem encountered during the manufacturing of a die casted component was porosity and the potential factors causing it are identified through causeeffect analysis. An analysis of variance (ANOVA) is conducted to find the factors with significant effects on porosity. The pre...

متن کامل

Computer-Aided System for Multi-Cavity Die-Casting Die-Design

Die-design for the die-casting process is a time consuming and complex activity that requires domain knowledge and vast experience of the die-designer besides information about manufacturing resources, part geometry, delivery time and cost preferences, etc. Complexity of the die-design activity further increases in case of a multi-cavity die. Currently available die-design systems lack in the l...

متن کامل

Study of Process Parameters of Gravity Die Casting Defects

In today’s world a casting production without any defect is almost impossible. After the application of various optimization techniques and process we still are not able to get the defect free castings. So it is critically important to analyze the root cause of casting defect with in the process itself, so that any changes which can hamper the defect intensity can be invoked at the time of manu...

متن کامل

Real-time Prediction and Synchronization of Business Process Instances using Data and Control Perspective

Nowadays, in a competitive and dynamic environment of businesses, organizations need to moni-tor, analyze and improve business processes with the use of Business Process Management Systems(BPMSs). Management, prediction and time control of events in BPMS is one of the major chal-lenges of this area of research that has attracted lots of researchers. In this paper, we present a...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Procedia Manufacturing

سال: 2020

ISSN: 2351-9789

DOI: 10.1016/j.promfg.2020.10.051