In this article, we report a new route to synthesize diamond by converting "solid" carbon nanofibers with a Spark Plasma Sintering system under low temperature and pressure (even at atmospheric pressure). Well-crystallized diamond crystals are obtained at the tips of the carbon nanofibers after sintering at 1500 °C and atmospheric pressure. Combining with scanning electron microscopy, transmiss...
متن کاملSynthesis of MgB2 at Low Temperature and Autogenous Pressure
High quality, micron-sized interpenetrating grains of MgB₂, with high density, are produced at low temperatures (~420 °C < T < ~500 °C) under autogenous pressure by pre-mixing Mg powder and NaBH₄ and heating in an Inconel 601 alloy reactor for 5-15 h. Optimum production of MgB₂, with yields greater than 75%, occurs for autogenous pressure in the range 1.0 MPa to 2.0 MPa, with the reactor at ~50...
متن کاملSynthesis of highly transparent ultrananocrystalline diamond films from a low-pressure, low-temperature focused microwave plasma jet
This paper describes a new low-temperature process underlying the synthesis of highly transparent ultrananocrystalline diamond [UNCD] films by low-pressure and unheated microwave plasma jet-enhanced chemical vapor deposition with Ar-1%CH4-10%H2 gas chemistry. The unique low-pressure/low-temperature [LPLT] plasma jet-enhanced growth even with added H2 and unheated substrates yields UNCD films si...
متن کاملGrowth of Single-walled Carbon Nanotubes at Low Temperature and Low Pressure Cvd Conditions
Controlling the detailed structures of single-walled carbon nanotubes (SWNTs) is imperative for realizing many SWNT applications, and understanding the SWNT growth mechanism is important to improve the growth techniques. In the present study, we performed SWNT growth by a catalytic chemical vapor deposition (CVD) method in wide temperature and pressure ranges, using a high-vacuum CVD chamber. W...
متن کاملLow temperature internal friction of diamond-like carbon films
We have studied the internal friction of amorphous diamond-like carbon films prepared by pulsed-laser deposition from 0.4 to 300K. The low temperature internal friction below 10K is dominated by the atomic tunnelling states for amorphous solids, which is a measure of structure disorder. We have tried to vary the content of sp carbon atoms versus sp ones by changing laser fleunce, by doping with...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Scientific Reports
سال: 2015
ISSN: 2045-2322
DOI: 10.1038/srep13879