Development and Evaluation of the Internal Cladding Process of API 5L X70 Risers with Nickel-based superalloy 625 via PTA Welding

نویسندگان

چکیده

The Oil and gas exploration is one of the most strategic industrial sectors in Brazilian economy. discovery deep water reserves adds more difficulty to already problematic use materials equipment extremely corrosive environments. With objective increasing service life equipment, consequently reducing cost maintenance preventing against environmental catastrophes, it common CRA claddings via welding processes, which nickel superalloy coatings stand out PTA process. In this context, operation internal cladding risers becomes complex due operational metallurgical requirements imposed by application. present work aims at development empirical evaluation procedure with Nickel-based 625 From tests on plate, satisfactory preliminary parameters were reached for performance risers. adaptation parameters, comparative analyzes three different procedures carried out, weaving amplitude. Visual analysis inspections penetrating liquid radiography, confirming quality all performed. Still, proving developed procedures, chemical composition was EDX, presenting results. Finally, a financial comparison process elaborated, showing comparatively consumption powder gas, time needed cladding.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

the evaluation of language related engagment and task related engagment with the purpose of investigating the effect of metatalk and task typology

abstract while task-based instruction is considered as the most effective way to learn a language in the related literature, it is oversimplified on various grounds. different variables may affect how students are engaged with not only the language but also with the task itself. the present study was conducted to investigate language and task related engagement on the basis of the task typolog...

15 صفحه اول

azerbaijans political development after the collapse of soviet union and implication on relation with the islamic republic of iran

در فصل اول این پایاین نامه در خصوص تاریخ کشور اذربایجان قبل و بعد از جدایی این کشور از ایران مورد بررسی قرار گرفته است ودر فصل دوم تحولات سیاسی این کشور بعد از 1991 و در واقع بعد از فروپاشی شوروی و دولتهایی که روی کار امدند در از جمله دولت ابولفضل ایلچی بیگ،دولت حیدر علی اف وبعد از او پسرش الهام علی اف و نگرش هرکدام از این دولتها به سیاسیت خارجی اذربایجان مورد اشاره قرار گرفته است.در ودر فصل سو...

Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets

Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb ...

متن کامل

Improving the Erosion Behavior of Inconel 625 Substrate by PTA-Deposited Stellite6/B4C Composite Cladding

The purpose of this study was to improve the erosion behavior of Inconel 625 alloy by plasma transferred arc-deposited stellite6/B4C composite cladding. For this purpose, 5 wt.% of boron carbide was added to the stellite6 clad. Phase analysis and microstructure evaluation were conducted by Optical Microscope, Field Emission Scanning Electron Microscope (FESEM), and Energy-dispersive Spectroscop...

متن کامل

the survey of the virtual higher education in iran and the ways of its development and improvement

این پژوهش با هدف "بررسی وضعیت موجود آموزش عالی مجازی در ایران و راههای توسعه و ارتقای آن " و با روش توصیفی-تحلیلی و پیمایشی صورت پذیرفته است. بررسی اسنادو مدارک موجود در زمینه آموزش مجازی نشان داد تعداد دانشجویان و مقاطع تحصیلی و رشته محل های دوره های الکترونیکی چندان مطلوب نبوده و از نظر کیفی نیز وضعیت شاخص خدمات آموزشی اساتید و وضعیت شبکه اینترنت در محیط آموزش مجازی نامطلوب است.

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materia-rio De Janeiro

سال: 2021

ISSN: ['1517-7076']

DOI: https://doi.org/10.1590/s1517-707620210001.1249