Determination of mechanical performance of glass fiber reinforced and elastomer filled polyamide 6 composites

نویسندگان

چکیده

In this study, the mechanical performances of neat Polyamide 6 (PA6) polymer, 20wt.% glass fiber reinforced PA6, and 8% SEBS elastomer with 20% PA6 composite were investigated. Composite materials first produced in form granules by using a twin-screw extruder. Later, test samples molded, accordance American Society Testing Materials (ASTM) standards, an injection molding technique. Mechanical parameters such as tensile strength, modulus, elongation at break, impact flexural modulus determined tensile, impact, bending tests. With addition reinforcement to polymer matrix, properties increased, while break strength decreased. For rubber additive, increased 177%, other values The fractured surface microstructure images obtained from tests examined scanning electron microscope.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Fiber Surface Treatment on Wear Characteristics of Carbon Fiber Reinforced Polyamide 6 Composites

Ozone modification method and air-oxidation were used for the surface treatment of polyacrylonitrile(PAN)-based carbon fiber. The surface characteristics of carbon fibers were characterized by X-ray photoelectron spectroscopy (XPS). The interfacial properties of carbon fiber reinforced polyamide 6 (CF/PA6) composites were investigated by means of the single fiber pull-out tests. As a result...

متن کامل

Tribological and Mechanical Behaviors of Polyamide 6/Glass Fiber Composite Filled with Various Solid Lubricants

The effects of polytetrafluoroethylene (PTFE), graphite, ultrahigh molecular weight polyethylene (UHMWPE), and their compounds on mechanical and tribological properties of glass-fiber-reinforced polyamide 6 (PA6/GF) were studied. The polymeric materials were blended using twin-screw extruder and subsequently injection molded for test samples. Mechanical properties were investigated in terms of ...

متن کامل

Creep Behavior of Basalt and Glass Fiber Reinforced Epoxy Composites

The creep behavior of basalt fiber reinforced epoxy (BFRE) and glass fiber reinforced epoxy (GFRE) composites was studied through tensile testing at high temperature. To study the effect of reinforcing epoxy, the micro glass powder (MGP) was added at various volume percentage into the epoxy resin in BFRE composites. The initial strain for all the specimens were evaluated and compared with each ...

متن کامل

Mechanical properties of woven glass fiber-reinforced composites.

The aim of this investigation was to measure the flexural and compressive strengths and the corresponding moduli of cylindrical composite specimens reinforced with woven glass fiber. Test specimens were made by light-curing urethane dimethacrylate oligomer with woven glass fiber of 0.18-mm standard thickness. Tests were conducted using four reinforcement methods and two specimen diameters. Flex...

متن کامل

effect of fiber surface treatment on wear characteristics of carbon fiber reinforced polyamide 6 composites

ozone modification method and air-oxidation were used for the surface treatment of polyacrylonitrile(pan)-based carbon fiber. the surface characteristics of carbon fibers were characterized by x-ray photoelectron spectroscopy (xps). the interfacial properties of carbon fiber reinforced polyamide 6 (cf/pa6) composites were investigated by means of the single fiber pull-out tests. as a result, it...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International advanced researches and engineering journal

سال: 2021

ISSN: ['2618-575X']

DOI: https://doi.org/10.35860/iarej.934740