Synthetic approach for precise formation of PtZn bimetallic nano-alloys is reported, which are highly active and selective towards propane dehydrogenation.
منابع مشابه
Silica-Supported Au–Ni Catalysts for the Dehydrogenation of Propane
Inspired by previous studies on model systems, a series of silica-supported Au–Ni catalysts were prepared and tested for the conversion of propane in the presence of hydrogen. The Au–Ni/SiO2 catalysts were prepared by successive impregnation, i.e. Ni was deposited first followed by Au. TEM/EDX results confirmed the presence of bimetallic Au–Ni nanoparticles. The dehydrogenation of propane to pr...
متن کاملAtomic layer deposition for nanofabrication and interface engineering.
Atomic layer deposition (ALD) provides a tool for conformal coating on high aspect-ratio nanostructures with excellent uniformity. It has become a technique for both template-directed nanofabrications and engineering of surface properties. This Feature Article highlights the application of ALD in selected fields including photonics, SERS and energy materials. Specifically, the topics include fa...
متن کاملNovel and Effective Copper–Aluminum Propane Dehydrogenation Catalysts
The importance of solid catalysts for converting petroand bulk chemicals is reflected in the sheer magnitude of their market size: catalysts sales topped nine billion dollars in 2009. This large value mirrors also the increasing academic interest in heterogeneous catalysis research. As far as bulk chemicals (such as ethene, propene, and their derivatives) are concerned, there is a strong demand...
متن کاملZnO modified ZSM-5 and Y zeolites fabricated by atomic layer deposition for propane conversion.
ZnO modified ZSM-5 and Y zeolites are synthesized by performing atomic layer deposition (ALD) of ZnO to HZSM-5 and HY using diethyl zinc and water as the precursors. The surface area and pore volume of ZSM-5 and Y zeolites are progressively reduced with the increasing number of ZnO ALD cycles. XRD and SEM characterization methods show that highly dispersed ZnO species are deposited on the inter...
متن کاملInterface Engineering through Atomic Layer Deposition towards Highly Improved Performance of Dye-Sensitized Solar Cells
A composite photoanode comprising ultralong ZnO nanobelts and TiO2 nanoparticles was prepared and its performance in dye-sensitized solar cells (DSSCs) was optimized and compared to the photoanode consisting of conventional TiO2 nanoparticles. The ultralong ZnO nanobelts were synthesized in high yield by a facile solution approach at 90°C followed by annealing at 500°C. The effect of the ratio ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Catalysis Science & Technology
سال: 2021
ISSN: ['2044-4761', '2044-4753']
DOI: https://doi.org/10.1039/d0cy01528h