Depth of cure and hardness of an indirect composite polymerized with three laboratory curing units
نویسندگان
چکیده
منابع مشابه
Depth of cure and hardness of an indirect composite polymerized with three laboratory curing units.
This study determined the hardness and curing depth of a light-activated indirect composite polymerized with three laboratory light-polymerizing units for the purpose of comparing the curing performance of the three units. A light-activated composite material for indirect application (Vita Zeta) was polymerized with three light-polymerizing units equipped with the following light sources: 1) on...
متن کاملDepth of cure and hardness of indirect composite materials polymerized with two metal halide laboratory curing units.
The purpose of this study was to evaluate the depth of cure and Knoop hardness of indirect composite materials polymerized with different laboratory curing units. Five composite materials designed for fixed restoration veneer (Artglass, Ceramage, Epricord, Prossimo, and Solidex) were filled into a cylindrical mold and then light-exposed by using the respective proprietary laboratory curing unit...
متن کاملHardness of composite resin polymerized with different light-curing units
Introduction: The degree of polymerization depends on the type of light-curing unit. The aim of this study was to compare the hardness of composite resin cured by LED and Halogen light curing units. Methods: In this experimental study, 20 cylindrical samples of Tetric Ceram composite were prepared. Half of them were cured with Ultralume 2 LED and the other half with Astralis 7 Halogen light ...
متن کاملHardness of composite resin polymerized with different light-curing units
Introduction: The degree of polymerization depends on the type of light-curing unit. The aim of this study was to compare the hardness of composite resin cured by LED and Halogen light curing units. Methods: In this experimental study, 20 cylindrical samples of Tetric Ceram composite were prepared. Half of them were cured with Ultralume 2 LED and the other half with Astralis 7 Halogen light cur...
متن کاملColor Stability of a Microhybrid Resin Composite Polymerized with LED and QTH Light Curing Units
Introduction: Discoloration of resin composites is a common reason for replacement of these restorations. The aim of this study was to eva-luate the influence of different light curing de-vices on color stability of a microhybrid resin composite. Materials and Methods: 80 disc-shaped speci-mens (8 mm in diameter, 2-mm height) were fabricated from filtek Z250 resin composite. Specimens wer...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Oral Science
سال: 2007
ISSN: 1880-4926,1343-4934
DOI: 10.2334/josnusd.49.25