Decoration of Vertically Aligned Carbon Nanotubes with Semiconductor Nanoparticles Using Atomic Layer Deposition

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Modeling and optimization of atomic layer deposition processes on vertically aligned carbon nanotubes

Many energy conversion and storage devices exploit structured ceramics with large interfacial surface areas. Vertically aligned carbon nanotube (VACNT) arrays have emerged as possible scaffolds to support large surface area ceramic layers. However, obtaining conformal and uniform coatings of ceramics on structures with high aspect ratio morphologies is non-trivial, even with atomic layer deposi...

متن کامل

Varying Phases of Alumina Nanowires Templated by Vertically Aligned Carbon Nanotubes Grown via Atomic Layer Deposition

Typically, alumina nanowires (NWs) are synthesized via physical evaporation, templated anodized aluminum oxide (AAO), or the vapor-liquid-solid (VLS) process [1,2,3]. All of these techniques have been shown to demonstrate successful growth of alumina NWs; however, in the cases where a facile method resulting in vertically aligned NWs is desired, many of these methods are difficult to integrate ...

متن کامل

Optimized Conditions for Catalytic Chemical Vapor Deposition of Vertically Aligned Carbon Nanotubes

Here, we have synthesized vertically aligned carbon nanotubes (VA-CNTs), using chemical vapor deposition (CVD) method. Cobalt and ethanol are used as the catalyst and the carbon source, respectively. The effects of ethanol flow rate, thickness of Co catalyst film, and growth time on the properties of the carbon nanotube growth are investigated. The results show that the flow rate of ethanol and...

متن کامل

optimized conditions for catalytic chemical vapor deposition of vertically aligned carbon nanotubes

here, we have synthesized vertically aligned carbon nanotubes (va-cnts), using chemical vapor deposition (cvd) method. cobalt and ethanol are used as the catalyst and the carbon source, respectively. the effects of ethanol flow rate, thickness of co catalyst film, and growth time on the properties of the carbon nanotube growth are investigated. the results show that the flow rate of ethanol and...

متن کامل

Membranes of vertically aligned superlong carbon nanotubes.

In the present work, we have developed a simple but effective method to prepare superlong vertically aligned carbon nanotubes (SLVA-CNT) and epoxy composite membranes, and we have demonstrated that various liquids, including water, hexane, and dodecane, can effectively pass through the SLVA-CNT membranes. These results were confirmed by molecular dynamics simulations. While the mechanical densi...

متن کامل