Pearlitic ductile cast iron: damaging micromechanisms at crack tip

Ductile cast irons (DCIs) are characterized by a wide range of mechanical properties, mainly depending on microstructural factors, as matrix microstructure (characterized by phases volume fraction, grains size and grain distribution), graphite nodules (characterized by size, shape, density and distribution) and defects presence (e.g., porosity, inclusions, etc.). Versatility and higher performa...

متن کامل

Microstructural characterization and kinetics modelization of vermicular cast irons

Several experimental techniques are used for phase identification and microstructure characterization of austempered vermicular cast irons (XRD, SEM, TEM and Mössbauer spectroscopy). Acicular structures were found to be composed by ferrite and austenite with average sizes compatible with those reported for bainitic ferrite in steels. An assessment of the free energy change involved in the auste...

متن کامل

Fatigue Behaviour of Synthetic Nodular Cast Irons

A. Vaško, L. Trško, R. Konečná, Faculty of Mechanical Engineering, University of Žilina, Žilina, Slovak Republic The paper shows the influence of charge composition on microstructure, fatigue properties and failure micromechanisms of nodular cast irons. The additive of metallurgical silicon carbide (SiC) in analysed specimens increases the content of ferrite in the matrix, decreases the size of...

متن کامل

Delamination Wear Mechanism in Gray Cast Irons

An investigation of the friction and sliding wear of gray cast iron against chromium plated cast irons was carried out on a newly constructed reciprocating friction and wear tester. The tests were the first to be done on the test rig under dry conditions and at the speed of 170 cm/min, and variable loads of 20-260 N for a duration of 15 min. to 3 hours. The gray cast iron surfaces worn by a pro...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Procedia Materials Science

سال: 2014

ISSN: 2211-8128

DOI: 10.1016/j.mspro.2014.06.051