Cyclic Fatigue Behavior of Superplastic Diffusion Bonded Y-TZP and Y-TZP/Alumina Composite
نویسندگان
چکیده
منابع مشابه
Fatigue sensitivity of Y-TZP to microscale sharp-contact flaws.
The strength degrading effects of sharp-contact damage are examined for Y-TZP ceramic plates bonded to a plastic substrate. Contacts are made with Vickers and Berkovich diamond indenters at low loads (0.1 N to 100 N) in the ceramic lower surfaces prior to bonding to the substrates. The indentations remain in the subthreshold region, that is, without visible corner radial cracks, over the lower ...
متن کاملBonding of Y-TZP to dentin: effects of Y-TZP surface conditioning, resin cement type, and aging.
PURPOSE To evaluate the effects of two surface treatments, aging, and two resin cements on shear bond strength between dentin and yttrium-stabilized tetragonal zirconia polycrystal ceramic (Y-TZP). MATERIALS AND METHODS Eighty human molars were embedded in acrylic resin and sectioned 3 mm below the occlusal plane. These teeth and 80 cylindrical Y-TZP specimens (height, 4 mm; diameter, 3.4 mm)...
متن کاملCad/cam Y-tzp–based Restorations
Tel: 504-619-8607 Fax: 504-619-8741 E-mail: [email protected] Prospective clinical studies are evaluating the long-term success of Y-TZP–based all-ceramic FPDs. Y-TZP–based infrastructures for crowns and FPDs present favorable physical, mechanical, and optical properties. Some Y-TZP–based restorative systems use CAD/CAM technology. Nevertheless, technicians should be able to employ traditiona...
متن کاملDeposition of Crystalline Hydroxyapatite Nanoparticles on Y-TZP Ceramic: A Potential Solution to Enhance Bonding Characteristics of Y-TZP Ceramics
Objectives Many advantages have been attributed to dental zirconia ceramics in terms of mechanical and physical properties; however, the bonding ability of this material to dental structure and/or veneering ceramics has always been a matter of concern. On the other hand, hydroxyapatite (HA) shows excellent biocompatibility and good bonding ability to tooth structure, with mechanically unstable ...
متن کاملPre-sintered Y-TZP sandblasting: effect on surface roughness, phase transformation, and Y-TZP/veneer bond strength
OBJECTIVES. Sandblasting is a common method to try to improve the Y-TZP/veneer bond strength of dental prostheses, however, it may put stress on zirconia surfaces and could accelerate the t→m phase transformation. Y-TZP sandblasting before sintering could be an alternative to improve surface roughness and bonding strength of veneering ceramic. The aim of this study was to analyze the effect of ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Ceramic Society of Japan
سال: 1994
ISSN: 0914-5400,1882-1022
DOI: 10.2109/jcersj.102.982