منابع مشابه
Divorced Pearlite in Steels
Steels containing large carbon concentrations are used particularly when a large hardness is required, for example in the manufacture of components such as bearings. This, however, makes it difficult to shape or machine the alloys during the process of component manufacture unless they are first heat–treated into a softened condition. One method of achieving this economically is to generate a m...
متن کاملExtremely Fine Pearlite by Continuous Cooling Transformation
An extremely fine, fully pearlitic structure with an interlamellar spacing 30–50 nm has been obtained during continuous cooling transformation at a rate as low as 0.1 C s, of the steel that is normally used to produce nanostructured bainite. The solutes cobalt and aluminium have been added to accelerate the rate of reaction and reduce the interlamellar spacing by increasing the free energy of t...
متن کاملMixed Diffusion–Controlled Growth of Pearlite in Binary Steel
A kinetic theory for the diffusion–controlled growth of pearlite is presented, which accounts simultaneously for diffusion through the austenite and via the transformation front. The simplified method abandons the need for mechanical equilibrium at the phase junctions and yet is able to explain experimental data on the growth rate of pearlite. Furthermore, unlike previous analyses, the deduced ...
متن کاملThe Effect of Interlamellar Distance in Pearlite on CGI Machining
Swedish truck industry is investigating the possibility for implementing the use of Compacted Graphite Iron (CGI) in their heavy duty diesel engines. Compared to the alloyed gray iron used today, CGI has superior mechanical properties but not as good machinability. Another issue that needs to be addressed when implementing CGI is the inhomogeneous microstructure when the cast component has diff...
متن کاملDiffusion–Controlled Growth of Pearlite in Ternary Steels
A theory for the diffusion–controlled growth of pearlite in steels containing manganese is presented and assessed in the light of experimental data. Given the overwhelmingly rapid diffusivity that a substitutional solute has within the transformation front, the growth rate is found to be dominated by diffusion parallel to the interface with austenite as the rate controlling step. The relevant i...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Transactions of the Iron and Steel Institute of Japan
سال: 1972
ISSN: 0021-1583,1881-1183