Crevice corrosion of nickel superalloy in deaerated chloride/sulphate solution at 90°C

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Combining the Ohmic Drop and Critical Crevice Solution Approaches to Rationalize Intermediate Attack in Crevice Corrosion

Crevice corrosion material loss is often most severe at intermediate distances into the crevice. This intermediate attack can be rationalized using the ohmic drop model of Pickering if and only if the material in question exhibits active/passive behavior in the crevice environment. Conventional theories that ascribe control of crevice corrosion to chemical changes exclusively cannot rationalize...

متن کامل

Joining of nickel-base superalloy single crystals

Introduction ................................................................................................................................1 Overview of Weldability of Nickel-Base Superalloys..................................................................1 Crystallography............................................................................................................................

متن کامل

Combining Rigorously Controlled Crevice Geometry and Computational Modeling for Study of Crevice Corrosion Scaling Factors

Microfabrication methods have been used to construct crevice formers of rigorously controlled gap and length. These have been used to study the IR-controlled crevice corrosion of Ni200 in 0.5 M H2SO4 to determine the effect of crevice gap ~G! on the position of the accelerated attack (xcrit) within the crevice. The experimental results were then compared to the results of computational studies....

متن کامل

The Role of Copper on the Crevice Corrosion Behavior of Nickel-Chromium-Molybdenum Alloys in Aggressive Solutions

The effect of Cu on the localized corrosion of Ni-Cr-Mo alloys has been investigated in hot saline solutions by comparing the behavior of N06059 and N06200 alloys, using electrochemical and surface analytical techniques. No measurable effect of copper on anodic film growth kinetics and passive film properties was detected and the breakdown and repassivation potentials of the alloys were very si...

متن کامل

Effect of Alloying Elements on Crevice Corrosion Inhibition of Nickel- Chromium-Molybdenum-Tungsten Alloys under Aggressive Conditions: An Electrochemical Study

The effects of Cr, Mo and W on the crevice corrosion of a number of commercial Ni-Cr-Mo (W) alloys in 1.0 mol/L NaCl were studied using the potentiodynamic-galvanostaticpotentiodynamic technique to measure film breakdown and repassivation potentials as well as protection temperatures. As expected, Cr is the key element determining resistance to crevice initiation but a substantial Mo alloy cont...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Physics: Conference Series

سال: 2017

ISSN: 1742-6588,1742-6596

DOI: 10.1088/1742-6596/786/1/012034