Creep testing on fiber reinforced sand
                    
                        
                            نویسندگان
                            
                            
                        
                        
                    
                    
                    چکیده
منابع مشابه
Creep Behavior of Basalt and Glass Fiber Reinforced Epoxy Composites
The creep behavior of basalt fiber reinforced epoxy (BFRE) and glass fiber reinforced epoxy (GFRE) composites was studied through tensile testing at high temperature. To study the effect of reinforcing epoxy, the micro glass powder (MGP) was added at various volume percentage into the epoxy resin in BFRE composites. The initial strain for all the specimens were evaluated and compared with each ...
متن کاملCreep of experimental short fiber-reinforced composite resin.
The purpose of this study was to investigate the reinforcing effect of short E-glass fiber fillers oriented in different directions on composite resin under static and dynamic loading. Experimental short fiber-reinforced composite resin (FC) was prepared by mixing 22.5 wt% of short E-glass fibers, 22.5 wt% of resin, and 55 wt% of silane-treated silica fillers. Three groups of specimens (n=5) we...
متن کاملCreep behavior of bagasse fiber reinforced polymer composites.
The creep behavior of bagasse-based composites with virgin and recycled polyvinyl chloride (B/PVC) and high density polyethylene (B/HDPE) as well as a commercial wood and HDPE composite decking material was investigated. The instantaneous deformation and creep rate of all composites at the same loading level increased at higher temperatures. At a constant load level, B/PVC composites had better...
متن کاملcreep behavior of basalt and glass fiber reinforced epoxy composites
the creep behavior of basalt fiber reinforced epoxy (bfre) and glass fiber reinforced epoxy (gfre) composites was studied through tensile testing at high temperature. to study the effect of reinforcing epoxy, the micro glass powder (mgp) was added at various volume percentage into the epoxy resin in bfre composites. the initial strain for all the specimens were evaluated and compared with each ...
متن کاملReview on Experimental Investigation on Polypropylene Fiber Reinforced Concrete with Artificial Sand
The paper presents review of research work experimental investigation on polypropylene fibre reinforced concrete and concrete with artificial sand. Use of fiber reinforce polymer in civil engineering increase rapidly. Various type of fiber is used such as glass, carbon, steel, asbestos, polyester and polypropylene. The various experimental investigations for determination of properties of polyp...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Japanese Geotechnical Society Special Publication
سال: 2016
ISSN: 2188-8027
DOI: 10.3208/jgssp.oth-04