Creep Strength of Co-Free Ni-Base Single Crystal Superalloys
نویسندگان
چکیده
منابع مشابه
Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys
Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...
متن کاملHigh Temperature Nanoindentation of Ni-base Superalloys
Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...
متن کاملTemperature and Orientation Dependence of Creep Damage of Two Ni-base Superalloys
Both polycrystalline (PC) and directionally-solidified (DS) Ni-base superalloys are commonly applied as turbine materials to primarily withstand creep conditions manifested in either marine-, airor land-based gas turbines components. The thrust for increased efficiency of these systems, however, translates into the need for these materials to exhibit considerable strength and temperature resist...
متن کاملOpen-Cellular Co-Base and Ni-Base Superalloys Fabricated by Electron Beam Melting
Reticulated mesh samples of Co-29Cr-6Mo alloy and Ni-21Cr-9Mo-4Nb alloy (625) and stochastic foam samples of Co-29Cr-6Mo alloy fabricated by electron beam melting were characterized by optical metallography, and the dynamic stiffness (Young's modulus) was measured by resonant frequency analysis. The relative stiffness (E/Es) versus relative density (ρ/ρs) plotted on a log-log basis resulted in ...
متن کاملCONSTITUTIVE MODELING OF CREEP OF SINGLE CRYSTAL SUPERALLOYS A Dissertation by SHARAT CHAND PRASAD
Constitutive Modeling of Creep of Single Crystal Superalloys. (August 2005) Sharat Chand Prasad, B.Tech., Indian Institute of Technology, Kanpur; M.S., Texas A&M University Chair of Advisory Committee: Dr. K. R. Rajagopal In this work, a constitutive theory is developed, within the context of continuum mechanics, to describe the creep deformation of single crystal superalloys. The constitutive ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Institute of Metals
سال: 2005
ISSN: 0021-4876
DOI: 10.2320/jinstmet.69.707